Publications
Sort:
Open Access Research paper Issue
Microstructure and mechanical properties of B4C/TC4 titanium matrix composites produced by laser directed energy deposition
Journal of Aeronautical Materials 2025, 45(6): 109-117
Published: 01 December 2025
Abstract PDF (9 MB) Collect
Downloads:8

B4C/TC4 titanium matrix composites are fabricated by laser-directed energy deposition(L-DED) to investigate the effect of B4C content on the microstructure and mechanical properties of the deposited layers. The results indicate that during the deposited process, B4C reacts in-situ with the TC4 matrix, generating TiC and TiB reinforcement phases. With the addition of B4C content, the hardness of the composites increases significantly, while the plasticity decreases accordingly. When the mass fraction of B4C is 0.2%, the precipitated phases of TiC and TiB exhibit the most uniform distribution. At this point, the composite achieves the highest strength while still maintaining good plasticity, demonstrating the optimal comprehensive mechanical properties. This performance optimization is mainly attributed to the synergistic effect of multiple strengthening mechanisms, including the load transfer effect of TiB phases with a high aspect ratio, the pinning effect of precipitated phases on grain boundaries and the resulting grain refinement.

Issue
Lattice structure and mechanical properties of TPMS prepared by selective laser melting
Acta Aeronautica et Astronautica Sinica 2025, 46(3)
Published: 15 February 2025
Abstract PDF (2.5 MB) Collect
Downloads:76

Triply Period Minimal Surface (TPMS) lattice structures have a wide range of lightweight design prospects due to their lightweight, high strength and energy absorption properties. However, they are difficult to manufacture using traditional methods. Using Ti-6Al-4V powder as the material, lattice samples with different porosities of Gyroidand Primitiveand solid tensile samples were fabricated by Selective Laser Melting (SLM) technique, and the mechanical propertiesand microstructure were analyzed. The results show that the mechanical properties of TPMS tend to decrease with the increase of porosity, and the plasticity of Primitive structure is better than that of Gyroid structure, but the overall strength is lower than that of Gyroid structure. The compressive yield strengthand tensile strength of TPMS lattice structure reach 498 MPaand 373.0 MPa, and the mechanical properties of TPMS lattice structure are better than those based on bar diameter class (boby-centered cubic, face-centered cubic), and the elongation of lattice structure is 2.8% to 14.0% higher than that of solid sample. The fracture modes of the both lattice structures area mixture of toughnessand brittleness. Porosityand unfused powder are present on the surface of the lattice structures, but these microscopic defects do not affect their failure mechanism. The tensile strengthand elongation of the solid tensile sample prepared under the same process parameters reach 1 050 MPaand 17.5%, which is superior to the mechanical properties of traditional cast Ti-6Al-4V alloy.

Issue
Quasi-in situ electron backscatter diffraction tensile test on deformation mechanisms of laser melting deposited Ti-3Cu alloy
Acta Aeronautica et Astronautica Sinica 2025, 46(22)
Published: 11 June 2025
Abstract PDF (94.5 MB) Collect
Downloads:4

Ti-Cu alloys exhibit excellent mechanical properties and corrosion resistance, making them promising candidates for biomedical and aerospace engineering applications. However, their deformation mechanisms remain poorly understood. Quasi-in situ tensile testing combined with Electron Backscatter Diffraction (EBSD) was employed to investigate the microstructural evolution of a Laser Melting Deposited (LMD) Ti-3Cu alloy fabricated via in situ alloying during room-temperature tensile deformation. The results demonstrated heterogeneous orientation rotations within localized regions of individual grains. Dislocations were primarily concentrated at grain and subgrain boundaries, accompanied by a progressive increase in the fraction of Low-Angle Grain Boundaries (LAGBs, 2°-15°) with increasing strain. Analysis of localized grain evolution revealed that α-grains with distinct crystallographic orientations and morphologies underwent non-uniform deformation, where macroscopic strain was accommodated through grain rotation and substructure formation. Quantitative Schmid factor analysis combined with slip trace characterization confirmed the dominance of the prismatic slip system in the Ti-3Cu alloy. These findings provide critical insights into the deformation mechanisms of laser-melting-deposited Ti-Cu alloys, offering guidance for their fabrication and application in advanced technologies.

Total 3