Mg/Al bimetal combines the advantages of both aluminum and magnesium and has broad application prospects in automotive, aerospace, weapons, digital products and so on. The compound casting has the characteristics of low cost, easy to achieve metallurgical combination and suitable for the preparation of complex bimetallic parts. However, bimetallic joint strength is low due to differences of physical properties between Al and Mg, oxide film on metallic surface and interfacial Al-Mg IMCs, which is closely related to the interfacial microstructure and properties. Therefore, how to control the interface of the bimetal to achieve performance enhancement is the focus and difficulty in this field. At present, there are mainly the following strengthening methods. First, the “zincate galvanizing” and “electrolytic polishing+anodic oxidation” technology were exert on the surface of Al alloy to remove and break the oxide film, which improved the wettability between Al and Mg. Second, the undesirable Al-Mg IMCs were reduce or elimination by adding the interlayers (Zn, Ni and Ni-Cu). Thirdly, the evolution process of interfacial microstructure was changed and fine strengthening phases were formed by adding Si element to Al alloy or rare earth element to Mg alloy. Fourthly, mechanical vibration and ultrasonic vibration were applied in the process of the filling and solidification to refine and homogenize the interfacial structure. Finally, some other methods, including secondary rolling, thermal modification, heat treatment and constructing exterior 3D morphology, also can be used to regulate the interfacial microstructure and compositions. The above strengthening methods can be used alone or in combination to achieve bimetallic strengthening. Finally, the future development direction of the Mg/Al bimetal is prospected, which provides some new ideas for the development and application of the Mg/Al bimetal.
- Article type
- Year
Open Access
Review
Issue
Open Access
Full Length Article
Issue
In this paper, the effect of the Si content on microstructure evolution, mechanical properties, and fracture behavior of the Al-xSi/AZ91D bimetallic composites prepared by compound casting was investigated systematically. The obtained results showed that all the Al-xSi/AZ91D bimetallic composites had a metallurgical reaction layer (MRL), whose thickness increased with increasing Si content for the hypoeutectic Al-Si/AZ91D composites, while the hypereutectic Al-Si/AZ91D composites were opposite. The MRL included eutectic layer (E layer), intermetallic compound layer (IMC layer) and transition region layer (T layer). In the IMC layer, the hypereutectic Al-Si/AZ91D composites contained some Si solid solution and flocculent Mg2Si+Al-Mg IMCs phases not presented in the hypoeutectic Al-Si/AZ91D composites. Besides, increasing Si content, the thickness proportion of the T layer increased, forming an inconsistent preferred orientation of the MRL. The shear strengths of the Al-xSi/AZ91D bimetallic composites enhanced with increasing Si content, and the Al-15Si/AZ91D composite obtained a maximum shear strength of 58.6 MPa, which was 73.4% higher than the Al-6Si/AZ91D composite. The fractures of the Al-xSi/AZ91D bimetallic composites transformed from the T layer into the E layer with the increase of the Si content. The improvement of the shear strength of the Al-xSi/AZ91D bimetallic composites was attributed to the synergistic action of the Mg2Si particle reinforcement, the reduction of oxidizing inclusions and the ratio of Al-Mg IMCs as well as the orientation change of the MRL.
京公网安备11010802044758号