Full Length Article | Open Access

Microstructure evolution, mechanical properties and fracture behavior of Al-xSi/AZ91D bimetallic composites prepared by a compound casting

Guangyu Li, Wenming Jiang( ), Feng Guan, Junwen Zhu, Yang Yu, Zitian Fan
State Key Laboratory of Materials Processing and Die & Mould Technology, School of Materials Science and Engineering, Huazhong University of Science and Technology, Wuhan 430074, China
Show Author Information

Abstract

In this paper, the effect of the Si content on microstructure evolution, mechanical properties, and fracture behavior of the Al-xSi/AZ91D bimetallic composites prepared by compound casting was investigated systematically. The obtained results showed that all the Al-xSi/AZ91D bimetallic composites had a metallurgical reaction layer (MRL), whose thickness increased with increasing Si content for the hypoeutectic Al-Si/AZ91D composites, while the hypereutectic Al-Si/AZ91D composites were opposite. The MRL included eutectic layer (E layer), intermetallic compound layer (IMC layer) and transition region layer (T layer). In the IMC layer, the hypereutectic Al-Si/AZ91D composites contained some Si solid solution and flocculent Mg2Si+Al-Mg IMCs phases not presented in the hypoeutectic Al-Si/AZ91D composites. Besides, increasing Si content, the thickness proportion of the T layer increased, forming an inconsistent preferred orientation of the MRL. The shear strengths of the Al-xSi/AZ91D bimetallic composites enhanced with increasing Si content, and the Al-15Si/AZ91D composite obtained a maximum shear strength of 58.6 MPa, which was 73.4% higher than the Al-6Si/AZ91D composite. The fractures of the Al-xSi/AZ91D bimetallic composites transformed from the T layer into the E layer with the increase of the Si content. The improvement of the shear strength of the Al-xSi/AZ91D bimetallic composites was attributed to the synergistic action of the Mg2Si particle reinforcement, the reduction of oxidizing inclusions and the ratio of Al-Mg IMCs as well as the orientation change of the MRL.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys
Pages 1944-1964

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Li G, Jiang W, Guan F, et al. Microstructure evolution, mechanical properties and fracture behavior of Al-xSi/AZ91D bimetallic composites prepared by a compound casting. Journal of Magnesium and Alloys, 2024, 12(5): 1944-1964. https://doi.org/10.1016/j.jma.2022.08.010

664

Views

7

Downloads

23

Crossref

32

Web of Science

28

Scopus

0

CSCD

Received: 05 April 2022
Revised: 27 July 2022
Accepted: 22 August 2022
Published: 25 September 2022
© 2022 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/) Peer review under responsibility of Chongqing University