In cold regions, the mechanical performance of steel‒concrete composite structures is significantly influenced by the environmental temperature. Extreme conditions can easily degrade the interfacial bond between concrete and steel, reducing the collaborative capacity of the steel tube and concrete, thereby compromising structural durability and seismic performance. Seismic actions can also cause local buckling in steel tube-confined concrete (STCC) columns and concrete crushing, posing a risk of overall structural failure if not rapidly repaired. The northwestern regions of China, characterized by high altitude, frequent extreme plateau weather, rugged terrain with harsh climates, large diurnal temperature variations, and high seismic activity, subject steel tube-confined concrete structures to far more extreme temperature effects and seismic actions than other regions. To enable the rapid repair of bridges under seismic loading in cold regions, it is critical to assess the seismic performance of earthquake-damaged steel tube-confined concrete structures under low-temperature conditions after reinforcement. This study investigates the seismic damage mechanisms of externally steel-reinforced earthquake-damaged steel tube-confined concrete columns under varying environmental temperatures. The results provide a valuable reference to inform the reinforcement and retrofitting of existing damaged structures and related research on steel tube-confined concrete structures in cold regions.
Low-cycle reversed loading tests were performed on six specimens of steel tube-confined concrete columns reinforced with external steel jackets under varying environmental temperatures (−40 ℃, −20 ℃, and 20 ℃).The six specimens were designed by varying the wall thickness of the external steel tube. To simulate seismic damage, the six specimens were subjected to low-cycle reversed loading at ambient temperature until failure. Damaged specimens were then reinforced by encasing the column base in an external steel jacket and filling the interlayer with high-strength micro-expansive concrete. These reinforced specimens were then tested under low-cycle reversed loading at varying environmental temperatures. The failure modes, horizontal bearing capacity, and ductility performance of the reinforced columns under ambient temperature conditions were compared with those of the original columns. The seismic performance indicators of the reinforced specimens, including failure modes, horizontal bearing capacity, ductility, stiffness degradation, and energy dissipation capacity, were comprehensively analyzed to assess the influence of external steel jacket thickness on seismic performance. The results elucidated the seismic damage mechanisms of externally steel-reinforced steel tube-confined concrete columns under different environmental temperatures.
Under ambient temperature conditions, damaged sections of steel tube-confined concrete columns were effectively strengthened by reinforcing them using a circular steel jacket filled with high-strength micro-expansive concrete. In the original column specimens, the plastic hinge zone appeared approximately 3 cm above the bottom of the steel tube near the stiffener; in the reinforced specimens, this zone shifted to approximately 3 cm below the top of the external steel jacket. This indicates that the external steel jacket reinforcement effectively enhanced the damaged section of the column, shifting the plastic hinge zone upward. As the plastic hinge zone moved from the column base to the top of the external steel jacket, the reinforced column’s horizontal bearing capacity increased by 19.8%, and its ductility improved by 8.0% compared to the original column. Under different environmental temperatures, the reinforced specimens’ failure mode was characterized by flexural compressive plastic hinge failure, with buckling occurring approximately 3 cm below the top of the external steel jacket. The degree of steel tube buckling deformation was more pronounced at ambient temperatures; however, reduced at low temperatures. The damage pattern of the core concrete showed noticeable cracks above the failure section, with the number of cracks increasing as the temperature decreased. The lower the environmental temperature, the more prone the reinforced column was to failure, and the greater the damage severity compared to specimens tested at ambient temperatures. Under low-temperature conditions, the maximum increase in the reinforced column’s horizontal bearing capacity was 22.7% higher than that at ambient temperature, whereas the displacement ductility coefficient decreased significantly, with a maximum reduction of 38.3%. Furthermore, the horizontal bearing capacity increased with the thickness of the external steel jacket. A significant increase in horizontal bearing capacity was observed in the low-temperature compared to the ambient-temperature specimens. Under low-temperature conditions, the pore water within the concrete froze, filling the internal voids of the material and notably enhancing initial stiffness. Because of the significant difference in thermal expansion coefficients between steel and concrete, an additional temperature-induced confinement effect was generated during temperature variations.
Low temperature significantly influenced the seismic performance of steel tube-confined concrete-reinforced columns. Environmental temperature and external steel jacket thickness affected the initial stiffness, horizontal bearing capacity, ductility, and energy dissipation capacity of the reinforced specimens to varying degrees, primarily due to temperature-induced additional confinement effects and material property variations. The ductility of steel tube-confined concrete columns was consistently lower under low-temperature conditions than under ambient temperature conditions. This reduction was attributed to the increased brittleness of core concrete and the accelerated development of cumulative damage in low-temperature environments. Increased external steel jacket thickness enhanced the confinement effect on the original column, thereby improving its horizontal bearing capacity and its ductility.
京公网安备11010802044758号