The paper study the interfacial mechanical properties and structural evolution mechanisms in 6061/AZ31B/6061 composite plates with and without Ni foil interlayers. For Ni-free interfaces, a continuous diffusion layer (3.5–4.0 µm) forms, dominated by brittle columnar Al12Mg17 intermetallic compounds (IMCs, 0.27–0.35 µm thick), which act as preferential crack initiation sites. In contrast, Ni foil implantation induces interfacial restructuring during hot rolling: Constrained deformation fragments the Ni foil into grid-like segments with "olive"-shaped cross-sections, embedded into Mg/Al matrices. These fragments (56% areal coverage) coexist with dispersed multiphase IMCs (Mg2Ni, Al3Ni, Mg3AlNi, Al12Mg17; 10–20 nm grains) at fragment edges, forming a hybrid interface of "willow-leaf" Al12Mg17 islands and nanoscale Mg2Ni/Al3Ni layers (15–25 nm). Hall-Petch analysis reveals the multiphase IMC interface exhibits 3.6 × higher "kd-1/2" strengthening contribution than single-phase Al12Mg17 systems, attributed to grain refinement (20 nm vs. 260 nm average grain size). Synergistic effects of mechanical interlocking, adhesion hierarchy (Ni-Al > Ni-Mg >Al-Mg), and nanoscale reinforcement collectively enhance peel strength by 78% without compromising bulk tensile properties.
Publications
- Article type
- Year
- Co-author
Article type
Year
Open Access
Full Length Article
Issue
Journal of Magnesium and Alloys 2025, 13(9): 4346-4363
Published: 02 September 2025
Downloads:0
Total 1
京公网安备11010802044758号