Experimental analysis on superelasticity of large-diameter NiTi-SMA bars under different heat treatment processes
Journal of Civil and Environmental Engineering 2026, 48(5): 52-59
Published: 01 October 2026
Abstract PDF (8.7 MB) Collect
Downloads:0

The addition of large-diameter hyperelastic NiTi shape memory alloy (NiTi-SMA) bars to damping elements has been demonstrated to achive effective self-centring capability. However, given the high sensitivity of SMA materials to temperature, it is important to note that different heat treatment processes can have a certain impact on the mechanical properties of NiTi-SMA bars. This, in turn, can result in varying degrees of influence on the energy dissipation and self-centering ability of dampers or supports containing NiTi-SMA bars. It is therefore essential to conduct a thorough investigation into the impact of diverse heat treatment processes on the mechanical properties of large-diameter NiTi-SMA bars. This article first conducted different heat treatment processes on seven Ni-59.9% at Ti bars with a working section diameter of nine mm, followed by amplified cyclic tensile tests to investigate the effects of different heat treatment processes on the stress-strain relationship, residual strain, energy dissipation capacity, and other properties of the specimens. The research results indicate that appropriate heat treatment can significantly improve the superelasticity of NiTi-SMA bars, with typical flag-shaped stress-strain curves. The present study investigates the effects of heat treatment temperature and duration on the properties of NiTi-SMA bars with a working diameter of nine mm. The results demonstrate that the optimal heat treatment process for these bars is 400 ℃ for 30 minutes. It is observed that as the heat treatment process approaches the optimal value, the energy dissipation capacity, secant stiffness, and equivalent damping ratio of the specimens exhibit increased stability.

Issue
Analysis of Shear Force Transfer Mechanism of Reinforced Concrete Beams Without Stirrups
Journal of South China University of Technology (Natural Science Edition) 2025, 53(12): 82-93
Published: 01 December 2025
Abstract PDF (9.3 MB) Collect
Downloads:1

To investigate the variation in shear force transfer mechanisms of reinforced concrete (RC) beams without stirrups, 9 rectangular-section and 27 T-section RC beams without stirrups were designed, fabricated, and tested. Displacements and strain data were collected using digital image correlation (DIC), displacement transducers, and strain gauges. Kinematic images of critical shear cracks were plotted, and the contributions of four shear transfer mechanisms-aggregate interlock, dowel action, residual tensile stress across cracks, and shear resistance of the uncracked compression zone-were quantified throughout the loading process. The evolution of these mechanisms during loading was analyzed. The results indicate that the number, development, and height of shear cracks exhibit a complex coupling effect on the four shear force transfer mechanisms; aggregate interlock generally reaches its maximum contribution at approximately 0.9 Pu (where Pu is the peak load), and its calculated shear resistance varies little with the shear-span ratio; however, its proportional contribution decreases as the shear-span ratio decreases; dowel action remains relatively stable throughout loading, yet its relative contribution diminishes as the overall shear capacity increases. Residual tensile stresses across cracks contribute primarily in the early loading stage and diminish to zero at peak load due to full crack development. The shear capacity provided by the uncracked compression zone is influenced by multiple factors, most notably the shear-span ratio-the shear capacity in beams with small shear-span ratios can be more than twice that in beams with large shear-span ratios. At peak load, aggregate interlock is the dominant shear force transfer mechanism in beams with larger shear-span ratios. However, as the shear-span ratio decreases, the contribution of the uncompressed concrete zone increases rapidly and becomes the predominant mechanism.

Total 2