The three-layer structure molybdenum-silicon high-temperature oxidation-resistant coating was prepared on selective laser melting Ta10W alloy by slurry sintering process. The microstructure and element distribution of the Ta10W alloy and coating were characterized by SEM and EDS. The tensile properties, microhardness of the Ta10W alloy and coating, and the coating bonding strength were tested. The results show that the coating of selective laser melting Ta10W alloy is divided into three layers: outer, sub-outer and inner layers. The outer layer is TaSi2 and MoSi2 phases, the sub-outer layer is TaSi2 phase and dispersed Ta5Si3 phase, and the inner layer is Ta5Si3 phase. The yield strength, tensile strength and uniform elongation of the coating and remove coating specimens are 639, 647 MPa, 13.6%, and 602 MPa, 675 MPa, 22.7%, respectively. Compared to the Ta10W alloy specimen, the uniform strain of the remove coating specimen is increased by 5.5%. The reason for this is that the thermal effect in the coating preparation process eliminates the residual stress of the Ta10W alloy formed by selective laser melting. The yield strength of the coated specimen is increased by 37 MPa due to the application of the coating. The microhardness of the outer layer, sub-outer layer, inner layer and Ta10W alloy were 550HV0.2, 1120HV0.2 , 534HV0.01 and 307HV0.2, respectively. The average coating bonding strength is 63 MPa, which is higher than that of the ceramic and high entropy alloy coatings. This is due to the fact that the three-layer coating has a good metallurgical bond to the Ta10W alloy.
- Article type
- Year
- Co-author
Open Access
Research paper
Issue
Open Access
Full Length Article
Issue
A large-scale fine-grained Mg-Gd-Y-Zn-Zr alloy plate with high strength and ductility was successfully prepared by multi-pass friction stir processing (MFSP) technology in this work. The structure of grains and long period stacking ordered (LPSO) phase were characterized, and the mechanical properties uniformity was investigated. Moreover, a quantitative relationship between the microstructure and tensile yield strength was established. The results showed that the grains in the processed zone (PZ) and interfacial zone (IZ) were refined from 50 µm to 3 µm and 4 µm, respectively, and numerous original LPSO phases were broken. In IZ, some block-shaped 18R LPSO phases were transformed into needle-like 14H LPSO phases due to stacking faults and the short-range diffusion of solute atoms. The severe shear deformation in the form of kinetic energy caused profuse stacking fault to be generated and move rapidly, greatly increasing the transformation rate of LPSO phase. After MFSP, the ultimate tensile strength, yield strength and elongation to failure of the large-scale plate were 367 MPa, 305 MPa and 18.0% respectively. Grain refinement and LPSO phase strengthening were the major strengthening mechanisms for the MFSP sample. In particularly, the strength of IZ was comparable to that of PZ because the strength contribution of the 14H LPSO phase offsets the lack of grain refinement strengthening in IZ. This result opposes the widely accepted notion that IZ is a weak region in MFSP-prepared large-scale fine-grained plate.
京公网安备11010802044758号