Abstract
Magnesium hydride (MgH2) is a promising solid-state hydrogen carrier, yet its practical application is hindered by sluggish kinetics and a high dehydrogenation temperature. Herein, Ni single atoms supported on N-doped carbon (Ni/NC) are constructed to clarify the catalytic roles of Ni and NC and the underlying interfacial mechanism. The nano-Mg@Ni/NC composite absorbs 6.12 wt% H2 within 1000 s at 200 °C and releases 6.42 wt% within 500 s at 325 °C, with absorption and desorption activation energies of 30.18 and 82.14 kJ mol-1, respectively. Its onset dehydrogenation temperature is 205 °C, and 97.8% of the initial capacity is retained after 10 cycles. DFT calculations reveal that interfacial electronic coupling at the Ni-N4/MgH2 interface drives charge transfer, weakens Mg-H bonds, and lowers the dehydrogenation energy barrier. These results distinguish Ni-N4 sites as electronic modulators and NC as a conductive support. HAADF-STEM/EDS and XPS analyses of the as-milled, hydrogenated, and dehydrogenated samples demonstrate highly dispersed Ni single atoms and largely preserved Ni-N4 features. This work establishes interfacial electronic coupling as an effective strategy for advanced Mg-based hydrogen storage.

京公网安备11010802044758号
Comments on this article