Discover the SciOpen Platform and Achieve Your Research Goals with Ease.
Search articles, authors, keywords, DOI, etc.
Through quality test, ultrasonic wave velocity test, static mechanical test, and dynamic compression test, the physical and static mechanical properties of geopolymer concrete after water immersion for 180 d were studied, and the effects of water saturation and impact load on the mechanical properties of geopolymer concrete were analyzed. The results show that the geopolymer concrete reaches the water-saturated state after water immersion for 180 d, and the ultrasonic wave velocity of geopolymer increases after water saturation, while the compressive strength, splitting tensile strength, and flexural strength decrease. Water saturation increases the strength and stiffness of geopolymer concrete under impact load, while reducing its deformation capacity, with no significant effect on its energy consumption characteristics. The dynamic compressive strength and dynamic elastic modulus of geopolymer concrete increase after water saturation, the dynamic peak strain and pre-peak toughness decrease, and the impact toughness exhibits no significant alteration. The dynamic increase factor (DIF) of geopolymer concrete increases significantly after water saturation, and the fractal dimension of fragments decreases. The Comité Euro-International du Béton (CEB) model can well predict the DIF of geopolymer concrete in the dry state, but significantly underestimates the DIF value of geopolymer concrete in the water-saturated state. Based on the test results, a DIF fitting formula for geopolymer concrete in a water-saturated state is proposed.

This is an open access article under the CC BY license (https://creativecommons.org/licenses/by/4.0/).
Comments on this article