BN/La–Al–Si–O composite ceramics were fabricated by hot-pressed sintering using hexagonal boron nitride (h-BN), lanthanum oxide (La2O3), aluminia (Al2O3), and amorphous silica (SiO2) as the raw materials. The effects of sintering temperature on microstructural evolution, bulk density, apparent porosity, and mechanical properties of the h-BN composite ceramics were investigated. The results indicated that La–Al–Si–O liquid phase was formed during sintering process, which provided an environment for the growth of h-BN grains. With increasing sintering temperature, the cristobalite phase precipitation and h-BN grain growth occurred at the same time, which had a significant influence on the densification and mechanical properties of h-BN composite ceramics. The best mechanical properties of BN/La–Al–Si–O composite ceramics were obtained under the sintering temperature of 1700 ℃. The elastic modulus, flexural strength, and fracture toughness were 80.5 GPa, 266.4 MPa, and 3.25 MPa·m1/2, respectively.
BN/La–Al–Si–O composite ceramics were fabricated by hot-pressed sintering using hexagonal boron nitride (h-BN), lanthanum oxide (La2O3), aluminia (Al2O3), and amorphous silica (SiO2) as the raw materials. The effects of sintering temperature on microstructural evolution, bulk density, apparent porosity, and mechanical properties of the h-BN composite ceramics were investigated. The results indicated that La–Al–Si–O liquid phase was formed during sintering process, which provided an environment for the growth of h-BN grains. With increasing sintering temperature, the cristobalite phase precipitation and h-BN grain growth occurred at the same time, which had a significant influence on the densification and mechanical properties of h-BN composite ceramics. The best mechanical properties of BN/La–Al–Si–O composite ceramics were obtained under the sintering temperature of 1700 ℃. The elastic modulus, flexural strength, and fracture toughness were 80.5 GPa, 266.4 MPa, and 3.25 MPa·m1/2, respectively.
This study was financially supported by the National Key Research and Development Program of China (No. 2017YFB0310400) and the National Natural Science Foundation of China (Nos. 52072089, 51672060, and 51832002).
This article is licensed under a Creative Commons Attribution 4.0 International License, which permits use, sharing, adaptation, distribution and reproduction in any medium or format, as long as you give appropriate credit to the original author(s) and the source, provide a link to the Creative Commons licence, and indicate if changes were made.
The images or other third party material in this article are included in the article’s Creative Commons licence, unless indicated otherwise in a credit line to the material. If material is not included in the article’s Creative Commons licence and your intended use is not permitted by statutory regulation or exceeds the permitted use, you will need to obtain permission directly from the copyright holder.
To view a copy of this licence, visit http://creativecommons.org/ licenses/by/4.0/.