Research Article | Open Access | Just Accepted

Sintering strategies govern grain and domain evolution for enhanced piezoelectric response in KNN-based lead-free ceramics

Fu Huang1, Wenfeng Yue1, Jian Dai1, Huazhan Gui1, Konstantin Nefedev2, Atilla Evcin3, Gulmurza Abdurakhmanov4, Nisrin Alnaim5, Adil Alshoaibi5( ), Dawei Wang1( )

1 Precision Acousto-optic Instrument Institute, School of Instrumentation Science and Engineering, Harbin Institute of Technology, Harbin 150080, China

2 Department of Theoretical Physics and Intelligent Technologies, Far Eastern Federal University, Vladivostok 690922, Russian

3 Materials Science and Engineering Department, Afyon Kocatepe University, Afyonkarahisar 03200, Türkiye

4 Faculty of Physics, The National University of Uzbekistan, Tashkent 100174, Uzbekistan

5 Department of Physics, College of Science, King Faisal University, Al-Ahsa 31982, Saudi Arabia

Show Author Information

Abstract

Lead-free potassium sodium niobate (KNN)-based piezoceramics are highly sensitive to sintering conditions, yet the microstructural origin of this processing dependence remains unclear. Here, a fixed-composition 0.96K0.48Na0.52Nb0.96Sb0.04O3–0.04Bi0.5Na0.5ZrO3 (KNNS-BNZ) ceramic was used to isolate the effect of sintering thermal history by comparing conventional sintering (CS), prolonged conventional sintering (PCS), and two-step sintering (TSS). The piezoelectric coefficient (d33) varies markedly with thermal history: CS at 1120 °C for 2 h yields approximately 260 pC/N, extending the dwell to 16 h increases d33 to 426 pC/N, and TSS at 1200 °C for 10 min followed by 1100 °C for 7 h further increases d33 to 493 pC/N. Across these representative states, the mean grain size increases from 0.77 to 2.11 and 6.57 μm, accompanied by stronger diffraction-peak splitting, larger tetragonal distortion, and a transition from fragmented domains to extended stripe-domain configurations. Polarization measurements further reveal that the coarse-grained TSS specimen retains a larger fraction of the field-induced polarization after field removal, consistent with its more stable remanent state. These results establish a thermal-history-driven processing–structure–property relationship in which grain coarsening and domain reorganization are closely associated with enhanced polarization retention and macroscopic piezoelectric response. This processing–structure–property relationship provides a practical route for optimizing KNN-based ceramics at fixed composition.

Graphical Abstract

Electronic Supplementary Material

Download File(s)
JAC1414-ESM.pdf (844 KB)

References

【1】
【1】
 
 
Journal of Advanced Ceramics

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Huang F, Yue W, Dai J, et al. Sintering strategies govern grain and domain evolution for enhanced piezoelectric response in KNN-based lead-free ceramics. Journal of Advanced Ceramics, 2026, https://doi.org/10.26599/JAC.2026.9221414

101

Views

13

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 04 October 2026
Revised: 02 November 2026
Accepted: 18 November 2026
Available online: 19 November 2026

© The Author(s) 2026.

The articles published in this open access journal are distributed under the terms of the Creative Commons Attribution 4.0 International License (http://creativecommons.org/licenses/by/4.0/).