AI Chat Paper
Note: Please note that the following content is generated by AMiner AI. SciOpen does not take any responsibility related to this content.
{{lang === 'zh_CN' ? '文章概述' : 'Summary'}}
{{lang === 'en_US' ? '中' : 'Eng'}}
Chat more with AI
PDF (15.6 MB)
Collect
Submit Manuscript AI Chat Paper
Show Outline
Outline
Show full outline
Hide outline
Outline
Show full outline
Hide outline
Research Article

Preparation and Performance of Al2O3/Glass‒Ceramic Composite Sealing Materials for Intermediate Temperature Solid Oxide Fuel Cell

Yunxiang SI1,2, Shangke PAN1, Haishen REN2( ), Huixing LIN2
Ningbo University, Ningbo 315211, Zhejiang, China
Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, China
Show Author Information

Abstract

To provide direction and guidance for the microstructure design and development of sealing materials for high-performance intermediate-temperature solid oxide fuel cell, a Al2O3/BaO–CaO–B2O3–Al2O3–SiO2 glass–ceramic (BCBAS)-based composite sealing material with superior mechanical properties and a high thermal conductivity was prepared via tape casting. According to the analysis by scanning electron microscopy and X-ray diffraction, the lamellar Al2O3 is regularly distributed in the BCBAS glass‒ceramic matrix. The main crystallization phase of BCBAS glass transforms from Ca0.1Ba0.9SiO3 into Ba1.55Ca0.45SiO4 and BaAl2Si2O8, and further into BaAl2Si2O8 and BaAl2O4 phases when the lamellar Al2O3 content increases from 0 to 25% (in mass fraction). The thermal conductivity of biomimetic sealants increases from 0.892 W/(m·K) to 1.255 W/(m·K), and the bending strength and Vickers hardness with higher than 10 of the Weibull modulus β increase from 96 MPa to 140 MPa and 444 HV to 677 HV as the lamellar Al2O3 content increases from 0 to 25% (in mass fraction), indicating the mechanical properties and thermal conductivity of the sealant. The sealing tensile strength of the biomimetic sealant with the mass fraction of lamellar Al2O3≤20% maintains above 4 MPa. The composite with 20% Al2O3–80% BCBAS glass exhibits the superior comprehensive properties (i.e., thermal conductivity of 1.203 W/(m·K), bending toughness of 136 MPa, Vickers hardness of 677 and sealing strength at 4.22 MPa), thus being a potential candidate for application of intermediate- temperature solid oxide fuel cell.

CLC number: O734 Document code: A Article ID: 0454-5648(2023)10-2653-09

References

【1】
【1】
 
 
Journal of the Chinese Ceramic Society
Pages 2653-2661

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
SI Y, PAN S, REN H, et al. Preparation and Performance of Al2O3/Glass‒Ceramic Composite Sealing Materials for Intermediate Temperature Solid Oxide Fuel Cell. Journal of the Chinese Ceramic Society, 2023, 51(10): 2653-2661. https://doi.org/10.14062/j.issn.0454-5648.20230293

602

Views

2

Downloads

0

Crossref

0

Web of Science

1

Scopus

Received: 04 May 2023
Revised: 17 May 2023
Published: 09 August 2023
© 2023 Journal of the Chinese Ceramic Society