Discover the SciOpen Platform and Achieve Your Research Goals with Ease.
Search articles, authors, keywords, DOl and etc.
The oxidation resistance of FGH4097, FGH4099, and a new Ni-based powder metallurgy (PM) superalloy FGHXX at 750-1100 ℃ is investigated by isothermal oxidation tests on the basis of FGH4095 and FGH4096 superalloys. Results show that the oxide layer of FGH4097 superalloy, mainly consist of Al2O3, become denser modestly with temperature rising without internal oxidation. Even after heating at 1100 ℃ for 200 h, the oxide layer is approximately only 10 μm. While the thickness of FGH4099 and FGHXX increase with temperature rising, but decrease at 1100 ℃ because of the oxide layer spallation. The surface of FGH4099 and FGHXX become layered above 900 ℃, which the inner side of both superalloys is Al2O3, and the outer side of FGH4099 superalloy is mainly Cr2O3, TiO2, Ta2O5, and Nb2O5, and that of FGHXX is mainly Cr2O3, TiO2, and Ta2O5 at 900 ℃ and 1000 ℃. While the outer side of both superalloys is comprised of (Ni, Co)Cr2O4 and Cr2O3 at 1100 ℃. The difference of oxide layer constitution and morphology comes from Al content discrepancy in five Ni-based PM superalloys. Therefore, the oxidation resistance from highest to lowest of the above five Ni-based PM superalloys is FGH4097>FGHXX≈FGH4099>FGH4095>FGH4096, which lays the theoretical and practical foundation to the material selection of components such as aero-engine turbine discs.
This is an open access article under the CC BY-NC license (http://creativecommons.org/licenses/by-nc/4.0/).
Comments on this article