Research paper | Publishing Language: Chinese | Open Access

Preparation and performance influence mechanism of alumina Z-pin reinforced Al2O3/Al2O3 ceramic matrix composite

Yuxiao SONG, Rui YANG, Hu LIU, Ce CHEN, Qiaosi ZHU, Jian JIAO( )
Ceramic Matrix Composites Research Division,AECC Beijing Institute of Aeronautical Materials,Beijing 100095,China
Show Author Information

Abstract

Al2O3/Al2O3 composites have attracted considerable attention as promising candidate materials for engine nozzle components, owing to their high specific strength and excellent long-term oxidation resistance. However, their weak interlaminar properties limit the range of potential applications. This study investigates Z-pin reinforcement technology and evaluates the performance of Al2O3/Al2O3 composites fabricated via slurry infiltration followed by hot-pressing sintering. Alumina-based Z-pins with a defect-free implantation depth over 3 mm are prepared using an alumina matrix slurry and alumina fibers, thereby enhancing the interfacial bonding strength between the Z-pins and the Al2O3/Al2O3 composite. Through an ultrasonic-assisted process, Z-pins are successfully inserted into alumina fiber prepregs, enabling the fabrication of Z-pin reinforced Al2O3/Al2O3 composites. The variations in mechanical properties under different processing parameters are systematically characterized. The results indicate that at a Z-pin spacing of 3 mm×3 mm, the interlaminar performance improves by over 20%. The bridging effect of the Z-pins along the thickness direction suppresses interlaminar crack propagation, shifting the failure mechanism from pure interfacial debonding between the matrix and fiber layers to a combined mode involving Z-pin fiber pull-out and matrix debonding. Meanwhile, the Z-pin implantation sites introduces “fish-eye” crack damage, which serves as initiation points for crack propagation and leads to a reduction in in-plane properties. Under the 3 mm×3 mm implantation pattern, tensile strength decreases by approximately 10%, and compressive strength declines by about 15%. Although Z-pin implantation induces some degree of in-plane performance degradation, it does not alter the overall failure mode of the composite, which continues to exhibit a ductile fracture tendency.

CLC number: V254 Document code: A Article ID: 1005-5053(2026)11-0069-08

References

【1】
【1】
 
 
Journal of Aeronautical Materials
Pages 69-76

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
SONG Y, YANG R, LIU H, et al. Preparation and performance influence mechanism of alumina Z-pin reinforced Al2O3/Al2O3 ceramic matrix composite. Journal of Aeronautical Materials, 2026, 46(11): 69-76. https://doi.org/10.11868/j.issn.1005-5053.2025.000197

1

Views

0

Downloads

0

Crossref

0

Scopus

0

CSCD

Received: 17 October 2025
Accepted: 03 December 2025
Published: 15 November 2026
© Journal of Aeronautical Materials 2026.

This is an open access article under the CC BY-NC license (http://creativecommons.org/licenses/by-nc/4.0/).