AI Chat Paper
Note: Please note that the following content is generated by AMiner AI. SciOpen does not take any responsibility related to this content.
{{lang === 'zh_CN' ? '文章概述' : 'Summary'}}
{{lang === 'en_US' ? '中' : 'Eng'}}
Chat more with AI
PDF (26.9 MB)
Collect
Submit Manuscript AI Chat Paper
Show Outline
Outline
Show full outline
Hide outline
Outline
Show full outline
Hide outline
Full Length Article | Open Access

High-strength Mg–Gd–Zn–Zr alloy with intragranular nano-precipitates mediated by hot-wire arc directed energy deposition

Jiayuan Cuia, Qifei Hana, Xinglong Dia, Yuanxuan Zhenga, Yueling Guoa( ), Rui Fub, Hanwen Xua, Wentao Xiea, En-Hou Hanc, Changmeng Liua( )
School of Mechanical Engineering, Beijing Institute of Technology, Beijing, 100081, China
Applied Mechanics Laboratory, Department of Engineering Mechanics, Mechano-X Institute, Tsinghua University, Beijing 100084, China
Institute of Corrosion Science and Technology, Guangzhou 510530, China

Peer review under the responsibility of Chongqing University.

Show Author Information

Abstract

To optimize the microstructure and the mechanical property, this work proposes a hot-wire arc directed energy deposition (HWA-DED) strategy for Mg–15Gd–1Zn–0.4Zr alloy (wt.%) by coordinating wire preheating with arc melting to reduce effective arc heat input. Compared with conventional wire-arc DED, HWA-DED yields refined grains (average size reduced from 9.0 ± 0.3 µm to 7.1 ± 0.2 µm), a higher fraction of high-angle grain boundaries, weaker texture, and a more uniform precipitation architecture. Three-dimensional X-ray microtomography and TEM reveal that HWA-DED produces finer and denser (Mg,Zn)3Gd precipitates with increased volume fraction (3.82% vs. 2.73%), along with lamellar LPSO structures and nanoscale zones that elevate dislocation density. Consequently, the as-deposited HWA-DED components exhibit higher hardness (113 HV vs. 86 HV) and significantly improved tensile strength while maintaining comparable ductility. For HWA-DED, the ultimate tensile strength (UTS), yield strength (YS), and elongation are 300 ± 5 MPa, 210 ± 4 MPa, and 7.0 ± 0.5% in the horizontal direction (H), and 302 ± 6 MPa, 214 ± 6 MPa, and 7.3 ± 0.4% in the vertical direction (V), respectively. For conventional WA-DED, these values are 260 ± 4 MPa, 192 ± 4 MPa, and 7.2 ± 0.1% (H), and 262 ± 6 MPa, 196 ± 6 MPa, and 7.5 ± 0.3% (V), respectively. Furthermore, fractography demonstrates a transition from quasi-cleavage in WA-DED to transgranular ductile tearing with deeper dimples in HWA-DED, which aligns well with the redistributed precipitates and the suppression of boundary-controlled damage. Ultimately, without requiring any post-process heat treatment, the HWA-DED strategy achieves a superior strength-ductility synergy for Mg–Gd–Zn–Zr alloys.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Cui J, Han Q, Di X, et al. High-strength Mg–Gd–Zn–Zr alloy with intragranular nano-precipitates mediated by hot-wire arc directed energy deposition. Journal of Magnesium and Alloys, 2026, 20. https://doi.org/10.1016/j.jma.2026.102133

2

Views

0

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 21 January 2026
Revised: 15 April 2026
Accepted: 06 May 2026
Published: 22 May 2026
© 2026 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/)