Full Length Article | Open Access

Through the extrusion temperature control AZ31B/6063 composite tubes microstructure to achieve strength-ductility synchronous enhancement

Peng Lia,b,c, Tao Wanga,b,c, Ke Chend, Yanjun Wanga,b,c, Hui Niua,b,c, Qingxue Huanga,b,c, Zhongkai Rena,b,c( )
College of Mechanical Engineering, Taiyuan University of Technology, Taiyuan 030024, China
State Key Laboratory of Metal Forming Technology and Heavy Equipment, Taiyuan, Shanxi 030024, China
Engineering Research Center of Advanced Metal Composites Forming Technology and Equipment of Ministry of Education, Taiyuan University of Technology, Taiyuan 030024, China
School of Mechanical and Aerospace Engineering, Jilin University, Changchun 130025, China

Peer review under the responsibility of Chongqing University.

Show Author Information

Abstract

In this study, AZ31B/6063 composite tubes were successfully prepared in the temperature range of 280–410 ℃ using an independently designed shear extrusion die, and the active regulation of the microstructure of the composite tubes was achieved by regulating the heat transfer process between the stem and the billet. Results indicate that composite tubes exhibit outstanding comprehensive mechanical properties at extrusion temperatures ranging from 280 to 380 ℃: tensile strengths consistently exceed 265 MPa, with synergistic elongation rates surpassing 20%. Notably, specimens extruded at 350 ℃ achieved a tensile strength of 280 MPa and an elongation rate of 20.5%. Microstructural analysis shows that the thin IMC layer at the interface, together with the fine-grained network structure formed on the magnesium alloy side, collectively facilitates strain transfer across the interface and inhibits stress concentration within the metal on one side, while the formation of local voids and microcracks at the interface releases local strain, thereby coordinating the deformation of the matrices on both sides to some extent. The synergistic interaction between the aforementioned microstructure and interfacial mechanisms enables the composite tube to maintain high strength while exhibiting significantly superior ductility compared to a single matrix, thereby achieving a simultaneous enhancement of strength and ductility.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Li P, Wang T, Chen K, et al. Through the extrusion temperature control AZ31B/6063 composite tubes microstructure to achieve strength-ductility synchronous enhancement. Journal of Magnesium and Alloys, 2026, 20. https://doi.org/10.1016/j.jma.2026.102111

4

Views

0

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 16 January 2026
Revised: 20 March 2026
Accepted: 21 April 2026
Published: 14 May 2026
© 2026 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/)