AI Chat Paper
Note: Please note that the following content is generated by AMiner AI. SciOpen does not take any responsibility related to this content.
{{lang === 'zh_CN' ? '文章概述' : 'Summary'}}
{{lang === 'en_US' ? '中' : 'Eng'}}
Chat more with AI
PDF (53 MB)
Collect
Submit Manuscript AI Chat Paper
Show Outline
Outline
Show full outline
Hide outline
Outline
Show full outline
Hide outline
Full Length Article | Open Access

Thermal deformation behavior and related deformation mechanisms of Mg–3Y alloy under shear–compression loading conditions

Xiaoqi Liua,b, Shouxing Zhangb, Jiaxu Zhangb, Ziqi Wangb, Nian Yanb, Xiuli Houa,c( ), Rui Luob( ), Tao Zhanga( )
School of Physics and Materials Science, Guangzhou University, Guangzhou, Guangdong 510006, China
School of Material Science and Engineering, Jiangsu University, Zhenjiang, Jiangsu 212013, China
Jiangsu Key Laboratory of Advanced Structural Materials and Application Technology, Nanjing Institute of Technology, Nanjing 211167, China

Peer review under the responsibility of Chongqing University

Show Author Information

Abstract

In this work, the shear–compression deformation behavior of Mg–3Y alloy was systematically investigated by physical and numerical simulation. During thermal deformation at 300 ℃–400 ℃ and strain rates of 0.001s-1–0.1s-1, the shear–compression samples (SCSs) demonstrate sustained work hardening capability, which is supported by the Mises equivalent stress–strain curves. Numerical simulation and microstructure analysis reveal that after thermal deformation, the SCS exhibits three typical deformation regions. The slot region (Region Ⅰ) is primary stress and strain concentration zone; next is the transition region (Region Ⅱ); while stress and strain in the cylindrical region (Region Ⅲ) are minimal. Microstructure and micro-texture analyses of the slot region indicate that at 300 ℃, plastic deformation is primarily dominated by 〈a〉 basal slip, with multiple deformation twins assisting in <c>-axis deformation. At 350 ℃, besides 〈a〉 basal slip, 〈a〉 prismatic slip also participates, meanwhile, the proportion of deformation twinning decreases. At 400 ℃, the deformation is dominated by 〈a〉 prismatic slip, and deformation twinning nearly disappear. Additionally, both the increase in temperature and the decrease in strain rate play a promoting role in the occurrence of dynamic recrystallization (DRX). At 300 ℃, twin-induced dynamic recrystallization (TDRX) occurs within gain interiors. At 350 ℃, discontinuous dynamic recrystallization (DDRX) becomes the dominant mode. Both the DDRX and continuous dynamic recrystallization (CDRX) are enhanced at 400 ℃. Overall, the shear–compression stresses contribute to increasing the work hardening capability, while Y solute atoms stabilize the deformation microstructure by promoting non-basal dislocation activation and strengthening inter-atomic bonding. This dual mechanism significantly impedes dislocation mobility, resulting in pronounced work hardening and a substantial delay in the progress of DRX in Mg–3Y alloy at elevated temperatures.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Liu X, Zhang S, Zhang J, et al. Thermal deformation behavior and related deformation mechanisms of Mg–3Y alloy under shear–compression loading conditions. Journal of Magnesium and Alloys, 2026, 19. https://doi.org/10.1016/j.jma.2026.102074

4

Views

0

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 12 October 2025
Revised: 04 February 2026
Accepted: 30 March 2026
Published: 27 April 2026
© 2026 Chongqing University.

This is an open access article under the CC BY license (http://creativecommons.org/licenses/by/4.0/)