Full Length Article | Open Access

Effect of Ca content in Mg melt on dealloying kinetics and microstructural evolution of Mg–Ti composites fabricated via liquid metal dealloying

Jee Eun Janga,b, Bo Hyun Parka,b, Hyun Jun Youna,b, In-Chul Choic, Soo-Hyun Jood( ), Sung Hyuk Parka,b( )
Department of Materials Science and Metallurgical Engineering, Kyungpook National University, Daegu 41566, Republic of Korea
Graduate School of Materials Science and Engineering, Kyungpook National University, Daegu 41566, Republic of Korea
School of Materials Science and Engineering, Kumoh National Institute of Technology, Gumi 39177, Republic of Korea
Department of Materials Science and Engineering, Dankook University, Cheonan 31116, Republic of Korea

Peer review under the responsibility of Chongqing University.

Show Author Information

Abstract

Liquid metal dealloying (LMD) has emerged as an effective technique for producing Mg–Ti composites with three-dimensional bicontinuous architectures, making them suitable for lightweight structural and biomedical applications. This study systematically examines the effect of Ca addition (1, 5, and 10 wt.%) to the Mg melt on the dealloying kinetics, microstructural evolution, and mechanical properties of Mg–Ti composites, using a Ti–Cu precursor. Increasing Ca content markedly accelerates dealloying, reducing the time for complete Cu removal from 40 min (Mg–1Ca) to 20 min (Mg–10Ca). The early-stage dealloying depth and the duration of rapid dissolution increase with Ca content, indicating a sustained dissolution rate. Post-dealloying analysis reveals progressive Ca incorporation into the Mg matrix, with retained contents of 0.4 wt.% (Mg–1Ca), 1.3 wt.% (Mg–5Ca), and 3.5 wt.% (Mg–10Ca). When Ca exceeds its solubility limit, a fine Mg2Ca intermetallic phase forms, primarily as a eutectic phase. Ca also refines the Ti matrix, reducing its average width from 2.2 µm (Mg–1Ca) to 1.9 µm (Mg–10Ca). Morphologically, low Ca levels promote fragmentation of the Ti matrix, while higher Ca facilitates partial reconnection of the matrix. These compositional and structural changes enhance mechanical performance. The Vickers hardness increases from 109 Hv (Mg–1Ca) to 117 Hv (Mg–5Ca) and 152 Hv (Mg–10Ca). Collectively, the findings confirm that Ca alloying in the Mg melt enhances both processing efficiency and composite performance by accelerating dealloying and controlling microstructural characteristics, thereby providing a versatile route for optimizing bicontinuous Mg–Ti composites fabricated via LMD.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Jang JE, Park BH, Youn HJ, et al. Effect of Ca content in Mg melt on dealloying kinetics and microstructural evolution of Mg–Ti composites fabricated via liquid metal dealloying. Journal of Magnesium and Alloys, 2026, 20. https://doi.org/10.1016/j.jma.2026.102053

2

Views

0

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 10 December 2025
Revised: 27 January 2026
Accepted: 05 March 2026
Published: 30 March 2026
© 2026 Chongqing University.