AI Chat Paper
Note: Please note that the following content is generated by AMiner AI. SciOpen does not take any responsibility related to this content.
{{lang === 'zh_CN' ? '文章概述' : 'Summary'}}
{{lang === 'en_US' ? '中' : 'Eng'}}
Chat more with AI
PDF (25.4 MB)
Collect
Submit Manuscript AI Chat Paper
Show Outline
Outline
Show full outline
Hide outline
Outline
Show full outline
Hide outline
Full Length Article | Open Access

The influence of heat-treatment on regulating the content and morphology of LPSO phase in Mg-Y-Al alloy and its strengthening mechanism at room temperature

Qinghai Provincial Key Laboratory of New Light Alloys, Qinghai Provincial Engineering Research Center of High Performance Light Metal Alloys and Forming, Qinghai University, Xining 810016, China
School of Material Science and Engineering, Shenyang University of Technology, Shenyang 110870, China

✩ Peer review under the responsibility of Chongqing University.

Show Author Information

Abstract

The LPSO phase can effectively enhance the mechanical properties of Mg alloys. To investigate the impact of different LPSO phase contents and morphologies on the mechanical properties and strengthening mechanisms of Mg-Y-Al alloys under room temperature deformation, this study prepared Mg-12Y-1Al (WA121) alloys containing Bulk-LPSO (B-LPSO), Lattice-LPSO (L-LPSO), and Needle-like LPSO (N-LPSO) with different contents through different heat-treatment processes. The results indicate that with the increase in heat treatment time, the contents of B-LPSO phases remain essentially unchanged, and the contents of L-LPSO and N-LPSO phases gradually increase. The increase in N-LPSO phase content is the most pronounced, with the highest content (7.29%) observed in the alloy treated for 4.5 h. Moreover, the alloy treated for 4.5 h exhibits the best mechanical properties, with ultimate tensile strength (UTS), tensile yield strength (TYS), and elongation (EL) values of 177 MPa, 139 MPa, and 4.27%, respectively. Compared to the as-cast alloy, UTS, TYS, and EL increased by 9.94%, 11.2%, and 27.1%, respectively. The study reveals that all three LPSO phases exhibit excellent dislocation hindering effects, effectively enhancing strength of the alloy. Additionally, the N-LPSO phase, due to its dense distribution, forms numerous dislocation channels within the grains, dispersing stress concentration within the grains to improve plasticity of the alloy. Furthermore, the interaction between the N-LPSO phase and the other phases in the alloy can also enhance plasticity of the alloy. Therefore, the alloy treated for 4.5 h demonstrates a synergistic improvement in strength and plasticity. Research has revealed that the precipitation mechanism of the N-LPSO phase in the as-cast WA121 alloy involves the formation of an Al-rich region adjacent to the needle-like Mg24Y5 phase. Subsequently, the Y element provided by the dissolving Mg24Y5 phase reacts with this region, ultimately leading to the formation of the needle-like LPSO phase.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys
Pages 4412-4429

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Ren Q, Mi J, Wang J, et al. The influence of heat-treatment on regulating the content and morphology of LPSO phase in Mg-Y-Al alloy and its strengthening mechanism at room temperature. Journal of Magnesium and Alloys, 2025, 13(9): 4412-4429. https://doi.org/10.1016/j.jma.2025.02.020

2

Views

0

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 14 October 2024
Revised: 04 February 2025
Accepted: 18 February 2025
Published: 27 March 2025
© 2025 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/)