AI Chat Paper
Note: Please note that the following content is generated by AMiner AI. SciOpen does not take any responsibility related to this content.
{{lang === 'zh_CN' ? '文章概述' : 'Summary'}}
{{lang === 'en_US' ? '中' : 'Eng'}}
Chat more with AI
PDF (20.2 MB)
Collect
Submit Manuscript AI Chat Paper
Show Outline
Outline
Show full outline
Hide outline
Outline
Show full outline
Hide outline
Full Length Article | Open Access

Direct bonding of AZ31B and ZrO2 induced by interfacial sono-oxidation reaction at a low temperature

Z.L. Lia,b,1, J. Wanga,b,1, S.L. Yia,b, X.G. Songa,b( ), J.H. Fua,b, Y. Shia,b, J.C. Fenga,b
State Key Laboratory of Precision Welding & Joining of Materials and Structures, Harbin Institute of Technology, Harbin 150001, China
Shandong Provincial Key Lab of Special Welding Technology, Harbin Institute of Technology at Weihai, Weihai 264209, China

1 These authors contributed equally to this work and should be considered co-first authors.

✩ Peer review under the responsibility of Chongqing University.

Show Author Information

Abstract

Recently, the presentation of the metal-ceramic composite structure design provides an alternative idea for the improvement of components service performance, while conventional methods for joining metals and ceramics have to involve a high heat input. However, due to the low melting point of magnesium alloys, the magnesium alloys-ceramics joining system necessitates a low joining temperature. Ultrasonic vibrations can induce numerous defects in the solid matrix, which can effectively promote atomic diffusion and metallurgical bonding between solid-phase interfaces at low temperatures. Thus, ultrasonic-assisted bonding is a highly promising method for achieving rapid and reliable joining between metals and ceramics without the use of interlayers. In this study, the direct bonding of AZ31B alloy with ZrO2 ceramic was successfully achieved at 200 °C. A polycrystal spinel MgAl2O4 with an average thickness of 55 nm was identified at the AZ31B/ZrO2 interface. The average shear strength of joints reached 30.47 MPa. Furthermore, the dynamic recrystallization of AZ31B and the oxygen-depletion behavior of ZrO2 during the bonding process were characterized to illustrate the contribution of ultrasonic vibration to joint bonding. Consequently, the solid interfacial sono-oxidation reaction is proposed to discuss the bonding mechanism of the joint in detail.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys
Pages 4316-4326

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Li Z, Wang J, Yi S, et al. Direct bonding of AZ31B and ZrO2 induced by interfacial sono-oxidation reaction at a low temperature. Journal of Magnesium and Alloys, 2025, 13(9): 4316-4326. https://doi.org/10.1016/j.jma.2024.12.013

3

Views

0

Downloads

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 10 September 2024
Revised: 01 December 2024
Accepted: 08 December 2024
Published: 22 January 2025
© 2025 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/)