Full Length Article | Open Access

Design multifunctional Mg–Zr coatings regulating Mg alloy bioabsorption

Zohra Benzartia,b( ), Sandesh Itania, José David Castroa, Sandra Carvalhoa, Ana Sofia Ramosa
University of Coimbra, CEMMPRE, ARISE, Department of Mechanical Engineering, Rua Luís Reis Santos, 3030-788, Coimbra, Portugal
Laboratory of Multifunctional Materials and Applications (LaMMA), Department of Physics, Faculty of Sciences of Sfax, University of Sfax, Soukra Road km 3.5, B.P. 1171, Sfax, 3000, Tunisia
Show Author Information

Abstract

Magnesium (Mg) alloys are widely used for temporary bone implants due to their favorable biodegradability, cytocompatibility, hemocompatibility, and close mechanical properties to bone. However, rapid degradation and inadequate strength limit their applicability. To overcome this, the direct current magnetron sputtering technique is employed for surface coating in Mg-based alloys using various zirconium (Zr) content. This approach presents a promising strategy for simultaneously improving corrosion resistance, maintaining biocompatibility, and enhancing strength without compromising osseointegration. By leveraging Mg’s inherent biodegradability, it has the potential to minimize the need for secondary surgeries, thereby reducing costs and resources.

This paper is a systematic study aimed at understanding the corrosion mechanisms of Mg–Zr coatings, denoted Mg-xZr (x = 0–5 at.%). Zr-doped coatings exhibited columnar growth leading to denser and refined structures with increasing Zr content. XRD analysis confirmed the presence of the Mg (00.2) basal plane, shifting towards higher angles (1.15°) with 5 at.% Zr doping due to lattice parameter changes (i.e., decrease and increase of “c” and “a” lattice parameters, respectively). Mg–Zr coatings exhibited “liquidphilic” behavior, while Young’s modulus retained a steady value around 80 GPa across all samples. However, the hardness has significantly improved across all samples’ coating, reaching the highest value of (2.2 ± 0.3) GPa for 5 at.% Zr. Electrochemical testing in simulated body fluid (SBF) at 37 ℃ revealed a significant enhancement in corrosion resistance for Mg–Zr coatings containing 1.0–3.4 at.% Zr. Compared with the 5 at.% Zr coating which exhibited a corrosion rate of 32 mm/year, these coatings displayed lower corrosion rates, ranging from 1 to 12 mm/year. This synergistic enhancement in mechanical properties and corrosion resistance, achieved with 2.0–3.4 at.% Zr, suggests potential ability for reducing stress shielding and controlled degradation performance, and consequently, promising functional biodegradable materials for temporary bone implants.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys
Pages 1461-1478

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Benzarti Z, Itani S, Castro JD, et al. Design multifunctional Mg–Zr coatings regulating Mg alloy bioabsorption. Journal of Magnesium and Alloys, 2024, 12(4): 1461-1478. https://doi.org/10.1016/j.jma.2024.04.009

533

Views

4

Downloads

12

Crossref

14

Web of Science

13

Scopus

0

CSCD

Received: 27 December 2023
Revised: 03 April 2024
Accepted: 06 April 2024
Published: 19 April 2024
© 2024 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/) Peer review under responsibility of Chongqing University