In-situ observation of twinning and detwinning in AZ31 alloy

Wu Gonga,b( )Ruixiao Zhengc,d( )Stefanus HarjoaTakuro KawasakiaKazuya AizawaaNobuhiro Tsujib,c
J-PARC Center, Japan Atomic Energy Agency, 2-4 Shirane Shirakata, Tokai, Naka, Ibaraki 319-1195, Japan
Center for Elements Strategy Initiative for Structural Materials, Kyoto University, Yoshidahonmachi, Sakyo-ku, Kyoto 606-8501, Japan
Department of Materials Science and Engineering, Kyoto University, Yoshida-honmachi, Sakyo-ku, Kyoto 606-8501, Japan
School of Materials Science and Engineering, Beihang University, Beijing 100191, China
Show Author Information

Abstract

Twinning and detwinning behavior of a commercial AZ31 magnesium alloy during cyclic compression–tension deformation with a total strain amplitude of 4% (±2%) was evaluated using the complementary techniques of in-situ neutron diffraction, identical area electron backscatter diffraction, and transmission electron microscopy. In-situ neutron diffraction demonstrates that the compressive deformation was dominated by twin nucleation, twin growth, and basal slip, while detwinning dominated the unloading of compressive stresses and subsequent tension stage. With increasing number of cycles from one to eight: the volume fraction of twins at -2% strain gradually increased from 26.3% to 43.5%; the residual twins were present after 2% tension stage and their volume fraction increased from zero to 3.7% as well as a significant increase in their number; and the twinning spread from coarse grains to fine grains involving more grains for twinning. The increase in volume fraction and number of residual twins led to a transition from twin nucleation to twin growth, resulting in a decrease in yield strength of compression deformation with increasing cycles. A large number of <c>-component dislocations observed in twins and the detwinned regions were attributed to the dislocation transmutation during the twinning and detwinning. The accumulation of barriers including twin boundaries and various types of dislocations enhanced the interactions of migrating twin boundary with these barriers during twinning and detwinning, which is considered to be the origin for increasing the work hardening rate in cyclic deformation of the AZ31 alloy.

References

【1】
【1】
 
 
Journal of Magnesium and Alloys
Pages 3418-3432

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Gong W, Zheng R, Harjo S, et al. In-situ observation of twinning and detwinning in AZ31 alloy. Journal of Magnesium and Alloys, 2022, 10(12): 3418-3432. https://doi.org/10.1016/j.jma.2022.02.002

448

Views

5

Downloads

57

Crossref

52

Web of Science

56

Scopus

13

CSCD

Received: 02 November 2021
Revised: 07 January 2022
Accepted: 06 February 2022
Published: 11 March 2022
© 2022 Chongqing University.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/) Peer review under responsibility of Chongqing University