Open Access

Metal oxide-doped Al2O3-based ceramic shells in DZ125 nickel-based superalloy investment casting modulate wettability and interfacial reactions

Baohong KOUa,b,c, Wentao ZHOUa,b,c, Jing OUYANGa,b,c( )
Department of Inorganic Materials, School of Minerals Processing and Bioengineering, Central South University, Changsha 410083, China
Hunan Key Lab of Mineral Materials and Application, Central South University, Changsha 410083, China
Engineering Research Center of Ministry of Education for Carbon Emission Reduction in Metal Resource Exploitation and Utilization, Central South University, Changsha 410083, China

Peer review under responsibility of Editorial Committee of CJA.

Show Author Information

Abstract

Reactions at the interface between DZ125 nickel-based superalloys and Al2O3-based ceramic shells during investment casting adversely affect the surfaces of the resultant castings. Here, the effects of incorporating metal oxide dopants (HfO2, Al2O3, and Cr2O3) on the shell surfaces were investigated. The influence of dopant types and content (0–8wt%) on wettability and reactions at the interface was comprehensively analyzed via the sessile drop approach, followed by evaluation of the products and mechanisms. The findings demonstrate that enhancing the dopant amount markedly decreased shell surface porosity and roughness, mitigating molten metal corrosion. At high dopant contents (2wt%–8wt%), the angle of contact between the alloy and the shell improved while the contact area decreased, concurrently reducing the formation of sand sticking defects and reaction products. Thermodynamic analyses reveal the following mechanisms: the HfO2 dopant enhanced the chemical stability of the shells and effectively suppressed interfacial reactions. Furthermore, the Al2O3 dopant moderately improved shell stability but did not completely suppress displacement reactions between Hf and Al2O3, and the Cr2O3 dopant increased reactivity yet promoted the formation of a protective HfO2 layer that curbed further reactions. These findings demonstrate that doping Al2O3-based ceramic shells with metal oxides effectively regulates alloy-shell interfacial reactions, enhancing alloy surface integrity while maintaining favorable wettability.

References

【1】
【1】
 
 
Chinese Journal of Aeronautics

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
KOU B, ZHOU W, OUYANG J. Metal oxide-doped Al2O3-based ceramic shells in DZ125 nickel-based superalloy investment casting modulate wettability and interfacial reactions. Chinese Journal of Aeronautics, 2026, 39(8). https://doi.org/10.1016/j.cja.2026.104129

5

Views

0

Crossref

0

Web of Science

0

Scopus

0

CSCD

Received: 19 May 2025
Revised: 12 June 2025
Accepted: 27 July 2025
Published: 26 February 2026
© 2026 The Author(s). Chinese Society of Aeronautics and Astronautics.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).