Full Length Article | Open Access

Effect of initial microstructure on performance and corrosion behavior of GH4169 superalloy joint produced by linear friction welding

Xiawei YANG, Tingxi MENG, Yu SU( ), Rui XU, Zhenguo GUO, Yaxin XU, Tiejun MA, Wenya LI
State Key Laboratory of Solidification Processing, School of Materials Science and Engineering, Northwestern Polytechnical University, Xi’an 710072, China

Peer review under responsibility of Editorial Committee of CJA

Show Author Information

Abstract

The pre-weld heat treatment was carried out to obtain different initial microstructures of the GH4169 superalloy, and then Linear Friction Welding (LFW) was performed. The effect of the pre-weld heat treatment on the microstructure evolution and mechanical properties of the joint was analyzed, and the joint electrochemical corrosion behavior as well as the hot corrosion behavior was studied. The results show that the joint hardness of Base Metal (BM) increases after pre-weld heat treatment, and the strengthening phases γ′ and γ″ further precipitate. However, the precipitation phases dissolve significantly in the Weld Zone (WZ) due to the thermal process of LFW. The corrosion resistance in BM is reduced after the pre-weld heat treatment, while it is similar in WZ with a slight decrease. The surface morphology of the BM and WZ can be generally divided into a loose and porous matrix and a scattered oxide particle layer after hot corrosion. The joint cross section exhibits a Cr-depleted zone with the diffusion of Cr to form an oxide film. The corrosion product mainly consists of Fe2O3/Fe3O4 as the outer layer and Cr2O3 as the inner layer.

References

【1】
【1】
 
 
Chinese Journal of Aeronautics

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
YANG X, MENG T, SU Y, et al. Effect of initial microstructure on performance and corrosion behavior of GH4169 superalloy joint produced by linear friction welding. Chinese Journal of Aeronautics, 2025, 38(3). https://doi.org/10.1016/j.cja.2024.09.002

656

Views

31

Crossref

44

Web of Science

45

Scopus

0

CSCD

Received: 05 April 2024
Revised: 29 June 2024
Accepted: 31 July 2024
Published: 04 September 2024
© 2024 Chinese Society of Aeronautics and Astronautics

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).