Full Length Article | Open Access

Laser-assisted grinding of RB-SiC composites: Laser ablation behavior and mechanism

Zhigang DONG, Wenchao SUN, Xintong CAI, Feng YANG, Yan BAO, Renke KANG, Dongjiang WU, Guangyi MA, Fangyong NIU ( )
Key Laboratory for Precision and Non-traditional Machining Technology of the Ministry of Education, School of Mechanical Engineering, Dalian University of Technology, Dalian 116024, China

Peer review under responsibility of Editorial Committee of CJA.

Show Author Information

Abstract

Laser ablation is an important process during Laser-Assisted Grinding (LAG) of hard and brittle materials. To realize controllable material removal during laser ablation of RB-SiC composites, ablation experiments under different Laser Energy Density (LAED) and LAG experiments are conducted. Evolution rules and mechanism of physical phase, ablation morphology and crack characteristics caused by laser irradiation are investigated. The forces of LAG and Conventional Grinding (CG) are compared. The results show that ablation surface changes from slight oxidation to obvious material removal with LAED increasing, and ablation depth increases gradually. The ablation products change from submicron SiO2 particles to nanoscale particles and floccule. High LAED promotes SiC decomposition and sublimation, which leads to the increase of C element. The SiC phase forms corrugated shape in recast layer and columnar shape in Heat Affected Zone (HAZ) at 56 J/mm2. The cold and heat cycle leads to formation of fishbone crack. For ablation specimen under 30 J/mm2, the grinding force can be reduced by a maximum of 39% and brittle damage region is reduced. The material removal and microcrack generated will significantly reduce the hardness and improve machinability, which can promote grinding efficiency.

References

【1】
【1】
 
 
Chinese Journal of Aeronautics
Pages 362-376

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
DONG Z, SUN W, CAI X, et al. Laser-assisted grinding of RB-SiC composites: Laser ablation behavior and mechanism. Chinese Journal of Aeronautics, 2024, 37(1): 362-376. https://doi.org/10.1016/j.cja.2023.10.018

1329

Views

43

Crossref

41

Web of Science

42

Scopus

2

CSCD

Received: 06 December 2022
Revised: 27 December 2022
Accepted: 01 February 2023
Published: 27 October 2023
© 2023 Chinese Society of Aeronautics and Astronautics.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).