AI Chat Paper
Note: Please note that the following content is generated by AMiner AI. SciOpen does not take any responsibility related to this content.
{{lang === 'zh_CN' ? '文章概述' : 'Summary'}}
{{lang === 'en_US' ? '中' : 'Eng'}}
Chat more with AI
Article Link
Collect
Show Outline
Outline
Show full outline
Hide outline
Outline
Show full outline
Hide outline
Full Length Article | Open Access

Microstructure, mechanical and fracture properties of friction stir welded 2195 Al-Li alloy joints

Guangda SUNa,b, Weizhao SUNc, Li ZHOUa,b( ), Sanfeng LUOb, Zili ZHANGb, Debo LIUc, Huiqiang WUc
State Key Laboratory of Advanced Welding and Joining, Harbin Institute of Technology, Harbin 150001, China
Shandong Provincial Key Laboratory of Special Welding Technology, Harbin Institute of Technology (Weihai), Weihai 264209, China
Beijing Institute of Astronautical Systems Engineering, Beijing 100076, China

Peer review under responsibility of Editorial Committee of CJA.

Show Author Information

Abstract

The 8 mm-thick 2195 Al-Li alloy joints were achieved by Friction Stir Welding (FSW). The microstructural evolution, temperature-dependent mechanical properties, and fracture properties were studied. The T1, δ′/β′ and θ′ precipitates were observed in the Base Metal (BM) and the Heat Affected Zone (HAZ). Most of the precipitates, except for re-precipitated δ′/β′ phases, were dissolved in the Nugget Zone (NZ). The tensile specimens that failed at cryogenic temperatures (–196 °C) had the maximum Ultimate Tensile Strength (UTS), and the fracture surface showed the inter-granular fracture characteristics. Compared to those at room temperature (25 °C), the decreasing tensile properties at high temperature (180 °C) were related to microstructure and strain hardening effects. The NZ presented the optimal fracture toughness, and the Crack Tip Opening Displacement (CTOD) was mutually dominated by microhardness and grain size. Analysis on Fatigue Crack Growth (FCG) rates indicates that the Thermal-Mechanically Affected Zone (TMAZ) exhibited the most superior fatigue resistance performance at stress intensity range below 17 MPa·m1/2 due to compressive residual stress and the crack closure effect. The fatigue fracture surfaces reveal that the crack propagation zone was characterized by the striations and secondary cracks. Also, inter-granular fracture behavior was responsible for the fastest FCG rates in the NZ.

References

【1】
【1】
 
 
Chinese Journal of Aeronautics
Pages 345-361

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
SUN G, SUN W, ZHOU L, et al. Microstructure, mechanical and fracture properties of friction stir welded 2195 Al-Li alloy joints. Chinese Journal of Aeronautics, 2024, 37(1): 345-361. https://doi.org/10.1016/j.cja.2023.10.017

1480

Views

33

Crossref

28

Web of Science

30

Scopus

1

CSCD

Received: 17 November 2022
Revised: 30 December 2022
Accepted: 21 February 2023
Published: 27 October 2023
© 2023 Chinese Society of Aeronautics and Astronautics.

This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/).