@article{ZHU2019, author = {Guangxiang ZHU and Qian FENG and Jinshan YANG and Jianbao HU and Hongda WANG and Yudong XUE and Qingliang SHAN and Shaoming DONG}, title = {Effect of BNNTs/matrix interface tailoring on toughness and fracture morphology of hierarchical SiCf/SiC composites}, year = {2019}, journal = {Journal of Advanced Ceramics}, volume = {8}, number = {4}, pages = {555-563}, keywords = {nanocomposites, interface, boron nitride nanotubes (BNNTs), toughness and toughening}, url = {https://www.sciopen.com/article/10.1007/s40145-019-0338-0}, doi = {10.1007/s40145-019-0338-0}, abstract = {A thin BN interphase is applied on BNNTs surface to tailor the interfacial bonding between BNNTs and SiC matrix in hierarchical SiCf/SiC composites. The thickness of BN interphase ranging from 10 to 70 nm can be optimized by chemical vapor deposition after BNNTs are in situ grown on SiC fiber surface. Without BN interphase, the fracture toughness of hierarchical SiCf/SiC composites can be impaired by 13.6% due to strong interfacial bonding. As long as BN interphase with 30-45 nm thickness is applied, the interfacial bonding can be optimized and fracture toughness of hierarchical composites can be improved by 27.3%. It implies that tailoring BNNTs/matrix interface by depositing a layer of BN interphase is in favor of activating energy dissipation mechanisms at nanoscale induced by BNNTs.} }