@article{WANG2026, 
author = {Wei WANG and Jiale SHI and Xuhe GAO and Rongsen HE and Xiaomei CHEN},
title = {Experimental Study on High-temperature Performance of Rubber-modified Asphalt Sealant Based on Composite Modification},
year = {2026},
journal = {Advanced Engineering Sciences},
volume = {58},
number = {6},
pages = {217-230},
keywords = {asphalt sealant, basalt fiber, composite modified asphalt, high-temperature performance, response surface analysis},
url = {https://www.sciopen.com/article/10.12454/j.jsuese.202500279},
doi = {10.12454/j.jsuese.202500279},
abstract = {ObjectiveRubber-modified asphalt sealants used in northeastern China exhibit adequate low-temperature crack resistance; however, insufficient high-temperature performance, resulting in excessive deformation, mechanical degradation, and debonding under summer conditions. This limitation highlights the need to develop sealants that simultaneously satisfy performance requirements across extreme temperature ranges. In this study, we address this challenge by incorporating styrene-butadiene-styrene (SBS) copolymer and basalt fiber (BFC) into rubber-modified asphalt and optimizing their proportions to enhance high-temperature stability while maintaining the low-temperature flexibility required under regional climatic conditions.MethodsA composite system was prepared using 20% rubber-modified asphalt as the base matrix supplemented with 7% dibutyl phthalate (DBP) as a fixed plasticizer to improve low-temperature flexibility. Response Surface Methodology (RSM) combined with Box-Behnken Design (BBD) was employed to optimize three key components: SBS(8%‒10%), furfural-extracted oil (FEO,13%‒16%), and basalt fiber (BFC,1%‒4%). Seventeen experimental formulations were subj ected to a two-stage high-shear mixing process, which involved initial SB S dispersion at 175-185 ℃ and 4500 r/min for 30 minutes, followed by BFC incorporation at 165-175 ℃ and 2000 r/min for ≤15 minutes to minimize fiber breakage. Performance evaluation included the assessment of physical properties, including the softening point based on ASTM D3 6, cone penetration using modified ASTM D5, and elastic recovery based on JT/T 740—2024, as well as comprehensive rheological characterization. Rheological assessments included temperature sweep tests (35-95 ℃, 10 rad/s, and 1% strain) to determine the complex shear modulus (G*) and phase angle (δ) using a dynamic shear rheometer; multiple stress creep and recovery (MSCR, ASTM D7405) tests at 64℃ under applied stresses of 0.1 kPa and 3.2 kPa to quantify the recovery rate (R) and nonrecoverable creep compliance (Jnr); and frequency sweep tests (0.1‒100.0 Hz, 1% strain) across 30‒80℃ to establish time-temperature superposition (TTS) master curves. Low-temperature performance was validated through cyclic tensile tests conducted at-20℃ under 100% strain based on JT/T 740—2024. The composite performance was benchmarked against two commercial low-temperature (-30℃) sealants.Results and Discussions RSM optimization produced highly significant models (R2&gt; 0.97 for all responses) and identified the optimal component proportions as 9.9% SBS,15.0% FEO, and 1.3% BFC. Validation tests confirmed close agreement between the experimental and predicted values: the softening point was 95.5℃ (predicted: 95.9℃; error: 0.33%), cone penetration was 123.77 (0.1 mm)(predicted: 122.9; error: 0.34%), and elastic recovery was 65.71% (predicted: 67.0%; error: 1.19%). The composite sealant satisfied all JT/T 740—2024 specifications for the-30℃ grade, including the critical requirements for low-temperature tensile performance. Rheological characterization revealed substantial improvements in high-temperature performance. Temperature sweep tests demonstrated superior G* retention in the composite sealant (Group c:81 kPa at 64℃) compared to the SBS-modified control (Group b: 60 kPa, +35.2%) and commercial products (Groups d/e: 79/60 kPa). Group c consistently exhibited lower δ values than the unmodified and commercial groups, indicating enhanced elasticity, while also demonstrating the slowest rate of G* reduction with increasing temperature. MSCR tests further confirmed the superior performance of the composite sealant: at an applied stress of 0.1 kPa, Group c achieved a recovery rate of 48.07%(compared to 35.5% for Group b, +35.3%) and a Jnr value of 2758.12 kPa-1(compared to 3254.1 kPa-1 for Group b, -15.2%); at 3.2 kPa, the recovery rate reached 15.28%(compared to 9.6% for Group b, +63.7%), whereas the Jnr value was 1989.74 kPa-1(compared to 2917.3 kPa for Group b, -31.8%). The commercial products of Group d exhibited increases of 18.7%-22.4% in Jnr compared to Group c under high-stress conditions. Frequency sweep tests validated the TTS principle, with the master curve of Group c (30℃ reference temperature) exhibiting the lowest slope (0.322 compared to 0.425 for Group b), indicating reduced sensitivity to frequency and temperature variations. At low frequencies, which simulated high-temperature conditions, Group c maintained the highest G* (approximately 103 Pa), exceeding that of the unmodified sealant by two orders of magnitude. At high frequencies, which simulated low-temperature conditions, G* of Group c remained elevated (approximately 105 Pa), confirming balanced rheological performance. SEM analysis revealed uniform BFC dispersion within the SBS-modified matrix, which formed a synergistic three-dimensional network that provided mechanical reinforcement through interfacial bonding, stress transfer, microcrack bridging, and energy dissipation while complementing the elastic network formed by SBS.ConclusionsComposite modification of rubber-modified asphalt with optimized SBS(9.9%) and basalt fiber (1.3%) using RSM effectively addresses the high-temperature performance deficiency while preserving the low-temperature crack resistance required for the climate in Northeast China. The composite sealant achieved a softening point of 95.5℃, a 35.2% increase in G at 64℃, superior MSCR recovery (48.07% at 0.1 kPa and 15.28% at 3.2 kPa), and reduced Jnr compared to SBS-modified asphalt, surpassing commercial low-temperature sealants by&gt;30% in key high-temperature performance metrics. It maintained its low-temperature flexibility, passing cyclic tensile tests at-20℃. The SBS elastomeric network and BFC reinforcing skeleton formed a dual-phase structure in which SBS enhanced elasticity and recovery, whereas the BFC 3D network provided mechanical reinforcement, flow inhibition, energy dissipation, and crack bridging. This approach overcomes the traditional tradeoff between high-temperature stiffness and low-temperature flexibility in asphalt sealants, providing a viable high-performance solution for durable pavement maintenance in regions experiencing extreme temperature variations through cost-effective and sustainable modification strategies.}
}