@article{Wang2026, 
author = {Baojie Wang and Dongliang Wang and Daokui Xu and Zishuo Chen and Shuo Wang},
title = {Effect of high-temperature aging treatment on strength enhancement of the as-cast Mg-8Li-6Zn-1Y (in wt.%) alloy},
year = {2026},
journal = {Journal of Magnesium and Alloys},
volume = {20},
keywords = {Mg-Li based alloy, Ⅰ-phase, Thermal aging, Precipitation, Mechanical behavior},
url = {https://www.sciopen.com/article/10.1016/j.jma.2026.102068},
doi = {10.1016/j.jma.2026.102068},
abstract = {Based on the microstructural evolution of an as-cast Mg-8Li-6Zn-1Y alloy after being performed high-temperature aging treatment at 300 ℃, 330 ℃, and 400 ℃, it reveals that nano-sized quasi-crystalline structured Ⅰ-phase particles are precipitated in α-Mg matrix, whereas the high density of MgLiZn particles present in β-Li matrix are mostly dissolved during thermal aging process. With increasing aging temperature and time, the size and quantity of precipitated Ⅰ-phase particles increase gradually. For differently aged samples, the hardness values of β-Li matrix phase increase from 75 HV to 115 HV during the initial aging for up to 1 h and then stabilize at 115 HV with further prolonging the aging time, whereas the hardness values of α-Mg matrix phase change slightly and vary from 62 HV to 70 HV. The maximum macro hardness values corresponding to peak-aged conditions of 300 ℃/16 h, 330 ℃/8 h, and 400 ℃/4 h are respectively 89 HV, 96 HV, and 87 HV. Tensile results demonstrate that the 330 ℃/8 h sample has the yield strength of 179 MPa and the ultimate tensile strength of 233 MPa, whereas those of as-cast sample are 116 MPa and 166 MPa, respectively. The main strengthening mechanism of high-temperature aged samples is attributed to the precipitation strengthening of nano-sized Ⅰ-phase particles and solid solution strengthening because of the dissolution of MgLiZn phase.}
}