@article{ZHAO2026, 
author = {Bida ZHAO and Tianchi SHEN and Xiong ZHU and Yunjie GUAN},
title = {Seismic performance of partially encased composite (PEC) steel-concrete columns with T-shaped sections},
year = {2026},
journal = {Journal of Civil and Environmental Engineering},
volume = {48},
number = {5},
pages = {1-12},
keywords = {steel-concrete composite column, T-shaped section column, lateral bearing capacity, flexural capacity, stiffness, ductility},
url = {https://www.sciopen.com/article/10.11835/j.issn.2096-6717.2025.068},
doi = {10.11835/j.issn.2096-6717.2025.068},
abstract = {The present study investigates the seismic performance of partially encased composite steel-concrete columns with T-shaped sections (abbreviated as T-PEC columns). Five T-PEC column specimens with different axial compression ratios and main steel component (MSC) configurations are tested under cyclic horizontal load. Furthermore, MSCs are available in various forms, including solid-web steel and honeycomb steel with openings in the steel web. Based on the test and finite element (FE) analysis results, the impact of steel web openings and the axial compression ratio on the seismic performance of T-PEC columns is investigated. The findings indicate that all T-PEC column specimens failed in proximity to the column base, exhibiting plastic softening of the steel flange and adjacent concrete crushing. This is indicative of a typical cross-section compression-bending failure mode. The load-displacement hysteresis curves of all specimens were full, with the hysteresis loops at the same loading level almost coinciding, indicating effective energy dissipation and load-bearing stability. Steel web openings degraded deformability, ductility, and energy dissipation capacity of T-PEC columns. As the axial compression ratio increased, the lateral stiffness and lateral resistance capacity of the T-PEC columns increased, but the deformability, ductility, and energy dissipation capacity decreased. Both the full-section plasticity method and numerical integration method provided reasonably accurate estimates of the flexural capacity of the T-PEC column sections under the action of compression-bending load.}
}