TY - JOUR AU - LI, Yue AU - DONG, Chao AU - DING, Jingxiang AU - NING, Zhe AU - LUO, Anran PY - 2026 TI - Effect of environmental humidity on the self-healing performance of damaged UHPC JO - Journal of Civil and Environmental Engineering SN - 2096-6717 SP - 45 EP - 51 VL - 48 IS - 5 AB - In order to investigate the influence of environmental humidity on the self-healing performance of damaged ultra-high-performance concrete (UHPC), pre-cracks were induced in the specimens by loading, and then the specimens were subjected to secondary curing in four different environments: continuous immersion, wet-dry cycling, natural curing, and air-tight isolation. Subsequently, a series of rigorous evaluations was conducted, encompassing compressive and flexural tests, along with ultrasonic testing. The self-healing performance of UHPC were evaluated based on several criteria, including its appearance, mechanical properties, compactness, and micro-morphology. The findings indicate that environmental humidity exerts a substantial influence on the self-healing performance of the specimens. The discrepancy in the self-healing rate across varying humidity environments can be attributed to the migration and transportation of water. In water-deficient environments (air-tight isolation and natural curing), no obvious healing products were observed at the cracks of the specimens, and the recovery rates of strength and compactness of the specimens were low. In water-saturated environments (wet-dry cycling and continuous immersion), abundant visible healing products were observed at the cracks in the specimens. These products were composed of calcium hydroxide (Ca(OH)2) and calcium silicate hydrate (C-S-H) gel and were capable of effectively repairing the cracks. The recovery rates of strength and compactness of the specimens were superior in these environments. The recovery rates of strength and compactness of the specimens increased with the damage degree of the specimens. In the continuous immersion environment, compared with the specimens with a damage degree of 70%, the specimens with a damage degree of 90% had an increase of 16.59% in compressive strength recovery rate, an increase of 11.19% in flexural strength recovery rate, and a maximum increase of 64.43% in compactness recovery rate. UR - https://doi.org/10.11835/j.issn.2096-6717.2025.085 DO - 10.11835/j.issn.2096-6717.2025.085