@article{Wang2026, 
author = {Cunlong Wang and Kun Li and Yigang Hu and He Xie and Wencai Liu and Liang Zhang and Guohua Wu},
title = {Heat treatment, tensile and creep behaviors of Mg-Gd-Y-Zr alloy by novel near-liquidus squeeze cast},
year = {2026},
journal = {Journal of Magnesium and Alloys},
volume = {19},
keywords = {Mg alloys, Mg-Gd-Y alloys, Near-liquidus squeeze casting, Creep, Precipitate-free zone (PFZ), β′ phase},
url = {https://www.sciopen.com/article/10.1016/j.jma.2026.102078},
doi = {10.1016/j.jma.2026.102078},
abstract = {The microstructure evolution during solution heat treatment, age hardening responses, and tensile behaviors under varied heat treatment states of an Mg-Gd-Y-Zr alloy (VW93K) processed by novel near-liquidus squeeze casting (NSC) were studied. Moreover, the compressive creep behavior and microstructural evolution of T6-treated VW93K alloys prepared via gravity casting (GC), conventional squeeze casting (SC), and NSC were investigated comparatively. Creep tests at 200–250 ℃ under 50–120 MPa revealed that steady-state creep rates increased gradually from GC to SC and NSC alloys, although remaining within the same order of magnitude. The consistent combination of stress exponents (n ≈ 2), grain size exponent (p ≈ 2), and activation energies (Q ≈ 73.4~99.1 kJ/mol) across all processing routes unequivocally identifies grain boundary diffusion accommodated by grain boundary sliding (GBS) as the rate-controlling mechanism. TEM observations reveal significant microstructural degradation during creep, characterized by precipitate coarsening and the transformation of spindle-like β′ into elongated, chain-like structures. This evolution is driven by the formation of β′F ’’bridging’’ connectors between β′ precipitates, which leads to a loss of coherency and pinning efficiency. Dynamic precipitate-free zone (PFZ) also observed, acting as softened pathways for localized strain accumulation and facilitating GBS. The results highlight a trade-off where the grain refinement inherent to NSC enhances room-temperature strength but compromises creep resistance due to accelerated grain-boundary mediated processes. Alloy design strategies, including stabilizing precipitates and introducing high-melting secondary phases at grain boundaries, are proposed to optimize both strength and creep resistance. These findings provide guidance for future design of creep resistant Mg-RE alloys and corresponded casting technologies.}
}