@article{Rani2026, 
author = {Kanika Rani and  Aarti and R.S. Kundu and  Pooja and Deepak Saini and Neetu Ahlawat},
title = {Impact of tunable oxygen vacancy on microstructure, conduction mechanism and dielectric properties of Y3+/Mg2+ modified calcium copper titanate ceramics},
year = {2026},
journal = {Journal of Magnesium and Alloys},
volume = {19},
keywords = {Oxygen vacancies, Cationic vacancies, Activation energy, Hopping mechanism},
url = {https://www.sciopen.com/article/10.1016/j.jma.2026.101985},
doi = {10.1016/j.jma.2026.101985},
abstract = {Pure CaCu3Ti4O12 and rare-earth co-doped Ca1-xYxCu2.95Mg0.05Ti4O12 (x = 0.02, 0.04, 0.06) ceramics were synthesized by conventional solid state reaction method. X-Ray Diffraction (XRD) peaks confirmed the CaCu3Ti4O12 phase formation accompanied by a minor CuO peak around 35.5°. X-Ray Photoelectron Spectroscopy (XPS) was employed to predict the concentration of oxygen vacancies (intrinsic factor) and elucidate the presence of variable oxidation states (Cu2+/Cu+ and Ti4+/Ti3+) in prepared compositions. Photoluminescence (PL) study revealed the presence of blue-UV emission peaks in all samples related to shallow defects whereas the blue-green emission attributed to oxygen vacancies (             V                      O                    ⋅        ,            V                      O                    ⋅      ⋅      ), Ti4+ ↔ Ti3+ transitions or deep defects. Field Emission Scanning Electron Microscopy (FESEM) revealed that the simultaneous doping of Y3+/Mg2+ at Ca2+/Cu2+ site reduced the grain size from 3.44 µm to 1.78 µm. Transmission Electron Microscopy (TEM) was utilized to determine the grain boundary thickness (tgb) and reduced from 5.06 nm to 2.14 nm for CCTO and CY6CM5TO ceramic. The impedance studies demonstrated that grain boundary resistance (Rgb) exceeds bulk resistance (Rg) in all prepared samples, which consequently favors the IBLC model (Rgb&gt;&gt;Rg). Moreover, the grain boundary resistance enhanced with increasing Y3+ contents and was reported to be order of 106 (Ω) in Ca0.94Y0.06Cu2.95Mg0.05Ti4O12 ceramics. It was observed that the simultaneous doping of Y3+/Mg2+ in CCTO host matrix tailored the electrical response of ceramics by improving the dielectric constant (ε’) values and minimizing dielectric losses (tanẟ). Ca0.94Y0.06Cu2.95Mg0.05Ti4O12 ceramic witnessed the lowest dielectric losses (tanẟ = 0.0079 at 323 K and 1 kHz) making it a promising material for energy storage applications.}
}