@article{SUN2026, 
author = {Xiaojing SUN and Jiahua WANG and Ding YUAN and Zeng ZHANG and Zhenlin YANG and Fengchun JIANG and Chao WEI},
title = {Suppressing interfacial cracks of additively manufactured copper/austenitic stainless steel heterostructures by controlling solidification mode through interfacial alloying},
year = {2026},
journal = {Chinese Journal of Aeronautics},
volume = {39},
number = {8},
keywords = {Additive manufacturing, Copper/stainless steel bimetallic structure, Interfacial alloying, Liquid metal embrittlement, Solidification mode},
url = {https://www.sciopen.com/article/10.1016/j.cja.2026.104144},
doi = {10.1016/j.cja.2026.104144},
abstract = {Liquid Metal Embrittlement (LME) cracks at Cu/Austenitic Stainless Steel (ASS) interfaces during additive manufacturing compromise structural reliability. This study proposes a novel strategy to suppress LME cracks by controlling the solidification mode of austenitic stainless steel through interfacial alloying. Using Laser-Directed Energy Deposition (LDED), Ti1 (1 wt% Ti6Al4V + 316L) and Ti3 (3 wt% Ti6Al4V + 316L) interlayers were introduced between the 316L substrate and CuSn10 deposited layer. While control samples (no interlayer) show severe LME cracks, Ti1/Ti3 interfaces remain crack-free. Thermodynamic calculations and microstructure analysis reveal Ti6Al4V addition shifts 316L’s solidification mode from Austenitic (A) to Austenitic-Ferritic (AF) or Ferritic-Austenitic (FA). Molten pool convection further promotes FA/F modes in the fusion zone, blocking liquid Cu penetration along grain boundaries. Ti-rich precipitates segregate in Cu-rich regions, reducing liquid Cu mobility and stress concentration. Tensile tests confirm fractures occur solely in CuSn10 deposits, indicating robust interfacial bonding strength. This interfacial alloying strategy enables crack-free, high-reliability Cu/steel heterostructures in additive manufacturing.}
}