@article{Peng2026, 
author = {Xinxin Peng and Wen Deng and Damin Zheng and Hua Huang and Yunzhang Lu and Wangyang Sun and Lin Zhang and Junhui Ran and Yu Zhou and Fangyang Liu and Bin Yang and Yongbo Yuan and Liming Ding and Yun Lin},
title = {Controlling the nucleation window via low-volume antisolvents with mixed boiling points for high-efficiency blade-coated perovskite solar cells},
year = {2026},
journal = {Nano Research},
keywords = {antisolvent, blade coating, crystallization kinetics, nucleation, perovskite solar cells},
url = {https://www.sciopen.com/article/10.26599/NR.2026.94909341},
doi = {10.26599/NR.2026.94909341},
abstract = {Despite the substantial progress achieved with spin-coated perovskite solar cells (PSCs), the demand for scalable, high-throughput, and low-cost manufacturing techniques remains unfulfilled, largely because spin-coating processes cannot be directly transferred to large-area fabrication, such as the inapplicable antisolvent flushing for blade-coating techniques. In this study, we propose a low-volume antisolvent strategy to control the nucleation and crystallization processes for blade-coated PSCs. The interaction between the antisolvent and N,N-dimethylformamide (DMF) facilitates the desolvation of the PbI2:DMF solvated phase, leading to the formation of higher-order iodoplumbate complexes. This antisolvent-induced desolvation effect kinetically accelerates perovskite nucleation and crystal growth, enabling room-temperature drying. Besides, we proved that the retention time of the low boiling point toluene (TL) and high boiling point dichlorobenzene (DCB) in the main solvent is dramatically different, which play an important role in controlling the supersaturation and hence the nucleation window during film drying. The combination of TL and DCB antisolvents enables uniform and compact perovskite films. Accordingly, the power conversion efficiencies (PCEs) of blade-coated PSCs based on Q-2D (BDA)MA4Pb5I16 and 3D Cs0.15FA0.85Pb(I0.95Br0.05)3 perovskites were improved from 15.30% to 18.36%, and from 22.67% to 23.88%, respectively. Furthermore, the promoted nucleation induced by the low-volume antisolvent widens the N2 flow processing window during film drying, significantly reducing the PCE variation caused by fluctuations in N2 flow velocity. This work provides a viable and economical strategy for designing perovskite ink with controllable crystallization, paving the way toward efficient PSCs via scalable fabrication techniques.}
}