@article{SONG2026, 
author = {Yuxiao SONG and Rui YANG and Hu LIU and Ce CHEN and Qiaosi ZHU and Jian JIAO},
title = {Preparation and performance influence mechanism of alumina Z-pin reinforced Al2O3/Al2O3 ceramic matrix composite},
year = {2026},
journal = {Journal of Aeronautical Materials},
volume = {46},
number = {11},
pages = {69-76},
keywords = {alumina Z-pin, Al2O3/Al2O3 composites, interlaminar reinforcement, pull-out failure},
url = {https://www.sciopen.com/article/10.11868/j.issn.1005-5053.2025.000197},
doi = {10.11868/j.issn.1005-5053.2025.000197},
abstract = {Al2O3/Al2O3 composites have attracted considerable attention as promising candidate materials for engine nozzle components, owing to their high specific strength and excellent long-term oxidation resistance. However, their weak interlaminar properties limit the range of potential applications. This study investigates Z-pin reinforcement technology and evaluates the performance of Al2O3/Al2O3 composites fabricated via slurry infiltration followed by hot-pressing sintering. Alumina-based Z-pins with a defect-free implantation depth over 3 mm are prepared using an alumina matrix slurry and alumina fibers,  thereby enhancing the interfacial bonding strength between the Z-pins and the Al2O3/Al2O3 composite. Through an ultrasonic-assisted process, Z-pins are successfully inserted into alumina fiber prepregs,  enabling the fabrication of Z-pin reinforced Al2O3/Al2O3 composites. The variations in mechanical properties under different processing parameters are systematically characterized. The results indicate that at a Z-pin spacing of 3 mm×3 mm, the interlaminar performance improves by over 20%. The bridging effect of the Z-pins along the thickness direction suppresses interlaminar crack propagation, shifting the failure mechanism from pure interfacial debonding between the matrix and fiber layers to a combined mode involving Z-pin fiber pull-out and matrix debonding. Meanwhile, the Z-pin implantation sites introduces “fish-eye” crack damage, which serves as initiation points for crack propagation and leads to a reduction in in-plane properties. Under the 3 mm×3 mm implantation pattern, tensile strength decreases by approximately 10%, and compressive strength declines by about 15%. Although Z-pin implantation induces some degree of in-plane performance degradation,  it does not alter the overall failure mode of the composite, which continues to exhibit a ductile fracture tendency.}
}