@article{Jiang2025, 
author = {Xianquan Jiang and Na yang and Jiangyang Yu and Ruihao Zhang and Kaihong Zheng and Jing Li and Bo Feng and Xiaowei Feng and Fusheng Pan},
title = {Control mechanism of Ni-foil on the interfacial structure and properties of the magnesium alumina laminated composite plate},
year = {2025},
journal = {Journal of Magnesium and Alloys},
volume = {13},
number = {9},
pages = {4346-4363},
keywords = {Mg/Al composite plate, Rolling, Interface Ni-foil, Microstructure, Performance},
url = {https://www.sciopen.com/article/10.1016/j.jma.2025.06.025},
doi = {10.1016/j.jma.2025.06.025},
abstract = {The paper study the interfacial mechanical properties and structural evolution mechanisms in 6061/AZ31B/6061 composite plates with and without Ni foil interlayers. For Ni-free interfaces, a continuous diffusion layer (3.5–4.0 µm) forms, dominated by brittle columnar Al12Mg17 intermetallic compounds (IMCs, 0.27–0.35 µm thick), which act as preferential crack initiation sites. In contrast, Ni foil implantation induces interfacial restructuring during hot rolling: Constrained deformation fragments the Ni foil into grid-like segments with "olive"-shaped cross-sections, embedded into Mg/Al matrices. These fragments (56% areal coverage) coexist with dispersed multiphase IMCs (Mg2Ni, Al3Ni, Mg3AlNi, Al12Mg17; 10–20 nm grains) at fragment edges, forming a hybrid interface of "willow-leaf" Al12Mg17 islands and nanoscale Mg2Ni/Al3Ni layers (15–25 nm). Hall-Petch analysis reveals the multiphase IMC interface exhibits 3.6 × higher "kd-1/2" strengthening contribution than single-phase Al12Mg17 systems, attributed to grain refinement (20 nm vs. 260 nm average grain size). Synergistic effects of mechanical interlocking, adhesion hierarchy (Ni-Al &gt; Ni-Mg &gt;Al-Mg), and nanoscale reinforcement collectively enhance peel strength by 78% without compromising bulk tensile properties.}
}