@article{Liu2025, 
author = {Yanxia Liu and Chenxing Wang and Yan Song and Zhenglong Li and Xinqiang Wang and Fulai Qi and Jian Chen and Yongfeng Liu and Mingxia Gao and Hongge Pan},
title = {Reduced graphene oxide/patronite composite as highly active catalyst precursors for enhancing the hydrogen desorption of MgH2},
year = {2025},
journal = {Journal of Magnesium and Alloys},
volume = {13},
number = {9},
pages = {4596-4609},
keywords = {Metallic V, MgS catalyst, Hydrogen desorption kinetics, Reversibility, Magnesium hydride, Solid-state hydrogen storage materials},
url = {https://www.sciopen.com/article/10.1016/j.jma.2025.03.014},
doi = {10.1016/j.jma.2025.03.014},
abstract = {Although MgH2 is widely deemed to be the most promising solid-state hydrogen storage materials for the medium-high temperature fuelcell applications expected in the near future, the high-temperature desorption and sluggish hydrogen absorption/desorption kinetics are the major challenges for its applications. Herein, reduced graphene oxide/patronite nanoparticle composite (rGO@VS4) is successfully synthesized using an ionic liquid (IL)-assisted hydrothermal method, and superior catalytic effects originated from the rGO@VS4 composite precursor towards the hydrogen storage reaction of MgH2 are systematically investigated. The VS4 reacts with MgH2 leads to the in-situ formed and uniformly scattered of metallic V and MgS during both ball-milling and the initial hydrogen desorption, and the synergic catalytic effect of metallic V and MgS facilitates the improved hydrogen desorption of MgH2. The MgH2–15 wt% rGO@VS4 composite starts releasing hydrogen at 180 °C and peaks at 220 °C, which is 145 °C and 128 °C lower than that of the Pristine MgH2, respectively. The energy required for H2 desorption from MgH2 is decreased to 63.8 kJ mol−1, 58.9 kJ mol−1 lower than that of the Pristine MgH2. Furthermore, the MgH2–15 wt% rGO@VS4 composite shows excellent cycling stability, of which reversible hydrogen capacity can stabilize at about 5.9 wt% with capacity retention of 98.2% at 300 °C for 100 cycles. This study provides a deeper insight into metallic V and MgS to enhance the hydrogen desorption of solid-state hydrogen storage materials and also offers a perspective for the construction of high-activity catalysts for solid-state hydrogen storage materials.}
}