@article{WEI2025, 
author = {Qulong WEI and Lihong JIANG and Zheng LIU and Lin ZHU and Lianhai FAN and Guangang WANG and Mingjie ZHAO and Zhenghua GUO},
title = {Lattice structure and mechanical properties of TPMS prepared by selective laser melting},
year = {2025},
journal = {Acta Aeronautica et Astronautica Sinica},
volume = {46},
number = {3},
keywords = {Ti-6Al-4V, Selective Laser Melting (SLM), Triply Periodic Minimal Surface (TPMS), mechanical properties, failure mechanism},
url = {https://www.sciopen.com/article/10.7527/S1000-6893.2024.30593},
doi = {10.7527/S1000-6893.2024.30593},
abstract = {Triply Period Minimal Surface (TPMS) lattice structures have a wide range of lightweight design prospects due to their lightweight, high strength and energy absorption properties. However, they are difficult to manufacture using traditional methods. Using Ti-6Al-4V powder as the material, lattice samples with different porosities of Gyroidand Primitiveand solid tensile samples were fabricated by Selective Laser Melting (SLM) technique, and the mechanical propertiesand microstructure were analyzed. The results show that the mechanical properties of TPMS tend to decrease with the increase of porosity, and the plasticity of Primitive structure is better than that of Gyroid structure, but the overall strength is lower than that of Gyroid structure. The compressive yield strengthand tensile strength of TPMS lattice structure reach 498 MPaand 373.0 MPa, and the mechanical properties of TPMS lattice structure are better than those based on bar diameter class (boby-centered cubic, face-centered cubic), and the elongation of lattice structure is 2.8% to 14.0% higher than that of solid sample. The fracture modes of the both lattice structures area mixture of toughnessand brittleness. Porosityand unfused powder are present on the surface of the lattice structures, but these microscopic defects do not affect their failure mechanism. The tensile strengthand elongation of the solid tensile sample prepared under the same process parameters reach 1 050 MPaand 17.5%, which is superior to the mechanical properties of traditional cast Ti-6Al-4V alloy.}
}