@article{Kim2025, 
author = {Dong Il Kim and Hee Bin Jeong and Jungmoon Lim and Hyeong Seop Jeong and Min Kyeong Kim and Sangyeon Pak and Sanghyo Lee and Geon-Hyoung An and Sang-Soo Chee and Jin Pyo Hong and SeungNam Cha and John Hong},
title = {A Practical Zinc Metal Anode Coating Strategy Utilizing Bulk h-BN and Improved Hydrogen Redox Kinetics},
year = {2025},
journal = {Energy & Environmental Materials},
volume = {8},
number = {2},
keywords = {aqueous zinc ion batteries, H+ ion insertion, hexagonal boron nitride, scattering, Zn metal anode},
url = {https://www.sciopen.com/article/10.1002/eem2.12826},
doi = {10.1002/eem2.12826},
abstract = {Achieving high-performance aqueous zinc-ion batteries requires addressing the challenges associated with the stability of zinc metal anodes, particularly the formation of inhomogeneous zinc dendrites during cycling and unstable surface electrochemistry. This study introduces a practical method for scattering untreated bulk hexagonal boron nitride (h-BN) particles onto the zinc anode surface. During cycling, stabilized zinc fills the interstices of scattered h-BN, resulting in a more favorable (002) orientation. Consequently, zinc dendrite formation is effectively suppressed, leading to improved electrochemical stability. The zinc with scattered h-BN in a symmetric cell configuration maintains stability 10 times longer than the bare zinc symmetric cell, lasting 500 hours. Furthermore, in a full cell configuration with α-MnO2 cathode, increased H+ ion activity can effectively alter the major redox kinetics of cycling due to the presence of scattered h-BN on the zinc anode. This shift in H+ ion activity lowers the overall redox potential, resulting in a discharge capacity retention of 96.1% for 300 cycles at a charge/discharge rate of 0.5 A g−1. This study highlights the crucial role of surface modification, and the innovative use of bulk h-BN provides a practical and effective solution for improving the performance and stability.}
}