@article{Liu2022, 
author = {Jin-Li Liu and Han-Feng Wu and Zhi-Bei Liu and Ying-Qiang Wu and Li Wang and Feng-Li Bei and Xiang-Ming He},
title = {Insight into the Effects of Cation Disorder and Surface Chemical Residues on the Initial Coulombic Efficiency of Layered Oxide Cathode},
year = {2022},
journal = {Journal of Electrochemistry},
volume = {28},
number = {11},
pages = {2219001},
keywords = {lithium layered oxide cathode, initial coulombic efficiency, surface chemical residues, Li/Ni cation disorder},
url = {https://www.sciopen.com/article/10.13208/j.electrochem.2219001},
doi = {10.13208/j.electrochem.2219001},
abstract = {Lithium layered oxide LiNi0.6Co0.2Mn0.2O2 (NCM622) is one of the most promising cathode materials in high-energy lithium-ion batteries for electric vehicles. However, one drawback for NCM622 is that its initial coulombic efficiency (ICE) is only about 87%, which is at least 6% lower than that of LiCoO2 or LiFePO4. In this work, we investigated the effects of surface chemical residues (e.g., LiOH and Li2CO3) and Li/Ni cation disorder resulted during the sintering on the ICE. We found that the ICE of the as-prepared samples could be boosted from 80.80% to 86.68% as the sintering temperatures were increased from 825 to 900 ℃. The corresponding Li/Ni cation disorder and surface chemical residues were also reduced with the increasing sintering temperatures. Furthermore, the ICE of the sample sintered at 825 ℃ could be enhanced by 3.57% after washing with HNO3 solution to remove the surface residues despite the Li/Ni cation disorder being increased. These results demonstrate that minimizing the amount of surface residuals and the degree of Li/Ni cation disorder through an appropriate sintering process and post-treatment technology is critical to achieve a high ICE and improve the electrochemical performances of NCM622.}
}