Review Article | Open Access

Progress and Challenges for Energy-Dense and Cost-Effective Anode-Free Lithium Metal Batteries

Songjie Li1, Feng Wu1,2, Tiande Chen1,2, Kaidi Kang1,2, Ruiqi Guo1,2, Chen Liu1, Yao Niu1, Aolei Gao2, Ran Zhao1,2, Xinran Wang1,2( ), Ying Bai1,2 ( ), Chuan Wu1,2 ( )
Beijing Key Laboratory of Environmental Science and Engineering, School of Materials Science & Engineering Beijing Institute of Technology, Beijing 100081, P. R. China
Yangtze Delta Region Academy of Beijing Institute of Technology, Jiaxing 314019, P. R. China
Show Author Information

Abstract

Anode-free lithium metal batteries (AFLMBs), comprising a simple anode collector and a complete lithium cathode, are designed to minimize safety hazards associated with active Li metals, improve energy density, and simplify battery production. However, due to the irreversible loss of active lithium and the limited active lithium on the anode side, it generally leads to a rapid capacity loss of AFLMBs after only a few cycles. To enhance the extended cycling stability of AFLMBs, a thorough investigation spanning from battery components to design principles is required. In this paper, the main factors affecting the lifetime of AFLMBs, such as the induced nucleation relationship between the collector type and deposited Li, the determinative factors of Li deposition and stripping, and the interaction of mechanical and physicochemical properties of solid electrolyte interface (SEI) with the morphological evolution of various lithium deposits were studied. Subsequently, potential approaches and avenues to enhance the extended cycling performance of AFLMBs were deliberated and proposed, including electrolyte formulation adjustment to form SEI layers that promote uniform deposition of Li, cathode compensation for additional active lithium, and lipophilic coating or collection design with low nucleation barrier. And the important role of advanced testing techniques in guiding the development of AFLMBs was summarized. Finally, the further development of AFLMBs is discussed and proposed. The purpose of this review is to deepen the comprehension of AFLMBs and contribute to achieving an unprecedented cycle life in future.

References

【1】
【1】
 
 
Energy Material Advances
Article number: 0168

{{item.num}}

Comments on this article

Go to comment

< Back to all reports

Review Status: {{reviewData.commendedNum}} Commended , {{reviewData.revisionRequiredNum}} Revision Required , {{reviewData.notCommendedNum}} Not Commended Under Peer Review

Review Comment

Close
Close
Cite this article:
Li S, Wu F, Chen T, et al. Progress and Challenges for Energy-Dense and Cost-Effective Anode-Free Lithium Metal Batteries. Energy Material Advances, 2025, 6: 0168. https://doi.org/10.34133/energymatadv.0168

822

Views

6

Downloads

68

Crossref

56

Web of Science

59

Scopus

0

CSCD

Received: 15 August 2024
Revised: 25 November 2024
Accepted: 06 December 2024
Published: 26 March 2025
© 2025 Songjie Li et al. Exclusive licensee Beijing Institute of Technology Press. No claim to original U.S. Government Works.

Distributed under a Creative Commons Attribution License (CC BY 4.0).